General
Property | Temperature | Value | Condition | Testing Standard | Thickness | Comment |
---|---|---|---|---|---|---|
Density | 1.4 g/cm³ Show Supplier Material materials with Density of 1.4 g/cm³ | dry | ISO 1183 | |||
Moisture absorption | 23 °C | 1.8 % Show Supplier Material materials with Moisture absorption of 1.8 % | 50%RH | ISO 62 | 2 mm | |
Water absorption | 6.4 % Show Supplier Material materials with Water absorption of 6.4 % | ISO 62 | 2 mm | immersion at 23°C |
Mechanical
Property | Temperature | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|---|
Elastic modulus | 7.3 GPa Show Supplier Material materials with Elastic modulus of 7.3 GPa | 50%RH | ISO 527-2/1A | 1mm/min | |
11.1 GPa Show Supplier Material materials with Elastic modulus of 11.1 GPa | dry | ISO 527-2/1A | 1mm/min | ||
Elongation | 3.5 % Show Supplier Material materials with Elongation of 3.5 % | dry | ISO 527-2/1A | 5mm/min | |
8 % Show Supplier Material materials with Elongation of 8 % | 50%RH | ISO 527-2/1A | 5mm/min | ||
Flexural modulus | 6.4 GPa Show Supplier Material materials with Flexural modulus of 6.4 GPa | 50%RH | ISO 178 | 2mm/min | |
9.8 GPa Show Supplier Material materials with Flexural modulus of 9.8 GPa | dry | ISO 178 | 2mm/min | ||
Flexural strength | 100 MPa Show Supplier Material materials with Flexural strength of 100 MPa | 50%RH | ISO 178 | 2mm/min | |
280 MPa Show Supplier Material materials with Flexural strength of 280 MPa | dry | ISO 178 | 2mm/min | ||
Impact strength, Charpy notched | -30 °C | 10 kJ/m² Show Supplier Material materials with Impact strength, Charpy notched of 10 kJ/m² | dry | ISO 179/1eA | |
-30 °C | 16 kJ/m² Show Supplier Material materials with Impact strength, Charpy notched of 16 kJ/m² | 50%RH | ISO 179/1eA | ||
23 °C | 14 kJ/m² Show Supplier Material materials with Impact strength, Charpy notched of 14 kJ/m² | dry | ISO 179/1eA | ||
23 °C | 21 kJ/m² Show Supplier Material materials with Impact strength, Charpy notched of 21 kJ/m² | 50%RH | ISO 179/1eA | ||
Impact strength, Charpy unnotched | 70 kJ/m² Show Supplier Material materials with Impact strength, Charpy unnotched of 70 kJ/m² | dry | ISO 179/1eU | -30°C | |
87 kJ/m² Show Supplier Material materials with Impact strength, Charpy unnotched of 87 kJ/m² | dry | ISO 179/1eU | 23°C | ||
90 kJ/m² Show Supplier Material materials with Impact strength, Charpy unnotched of 90 kJ/m² | 50%RH | ISO 179/1eU | -30°C | ||
100 kJ/m² Show Supplier Material materials with Impact strength, Charpy unnotched of 100 kJ/m² | 50%RH | ISO 179/1eU | 23°C | ||
Tensile strength | 115 MPa Show Supplier Material materials with Tensile strength of 115 MPa | 50%RH | ISO 527-2/1A | 5mm/min | |
180 MPa Show Supplier Material materials with Tensile strength of 180 MPa | dry | ISO 527-2/1A | 5mm/min |
Thermal
Property | Value | Testing Standard | Comment | ||
---|---|---|---|---|---|
Heat deflection temperature | 200 °C Show Supplier Material materials with Heat deflection temperature of 200 °C | ISO 75/2Af | 1.80 MPa | ||
Melting point | 220 °C Show Supplier Material materials with Melting point of 220 °C | ISO 11357-1/-3 | 10°C/min | ||
Flammability | Automotive Interior Flammability(mm/min): 0 ,method: ISO 3795 and thickness tested (mm): 3 |
Electrical
Property | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|
Surface resistivity | 1e+12 Ω/sq Show Supplier Material materials with Surface resistivity of 1e+12 Ω/sq | dry | IEC 60093 | 500V |
Volume resistivity | 1e+13 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+13 Ω·cm | dry | IEC 60093 | 500V |
Technological properties
Property | ||
---|---|---|
Additives | Release agent | |
Certifications | RoHS 2011/65/UE | |
Color | Black | |
Features | DPPD Free | |
Fillers | 35% Glass Fiber | |
Processing methods | Injection Molding |