General
Property | Value | Testing Standard |
---|---|---|
Density | 1.59 g/cm³ Show Supplier Material materials with Density of 1.59 g/cm³ | ISO 1183 |
Mechanical
Property | Temperature | Value | Testing Standard | Comment |
---|---|---|---|---|
Elastic modulus | 12.8 GPa Show Supplier Material materials with Elastic modulus of 12.8 GPa | ISO 527-2/1A | 1mm/min | |
Elongation | 2.1 % Show Supplier Material materials with Elongation of 2.1 % | ISO 527-2/1A | 5mm/min | |
Flexural modulus | 14.2 GPa Show Supplier Material materials with Flexural modulus of 14.2 GPa | ISO 178 | 2mm/min | |
Flexural strength | 285 MPa Show Supplier Material materials with Flexural strength of 285 MPa | ISO 178 | 2mm/min | |
Impact strength, Charpy notched | 23 °C | 10 kJ/m² Show Supplier Material materials with Impact strength, Charpy notched of 10 kJ/m² | ISO 179/1eA | |
Impact strength, Charpy unnotched | 23 °C | 54 kJ/m² Show Supplier Material materials with Impact strength, Charpy unnotched of 54 kJ/m² | ISO 179/1eU | |
Impact strength, Izod notched | 23 °C | 11 kJ/m² Show Supplier Material materials with Impact strength, Izod notched of 11 kJ/m² | ISO 180/1A | |
Tensile strength | 190 MPa Show Supplier Material materials with Tensile strength of 190 MPa | ISO 527-2/1A | 5mm/min |
Thermal
Property | Value | Testing Standard | Comment | ||
---|---|---|---|---|---|
Heat deflection temperature | 260 °C Show Supplier Material materials with Heat deflection temperature of 260 °C | ISO 75/2Af | 1.80 MPa | ||
270 °C Show Supplier Material materials with Heat deflection temperature of 270 °C | ISO 75/2Bf | 0.45 MPa | |||
Melting point | 280 °C Show Supplier Material materials with Melting point of 280 °C | ISO 11357-1/-3 | 10°C/min | ||
Flammability | Thickness tested (mm): 0.8, Class: V-0, Standard: UL 94 |
Electrical
Property | Value | Testing Standard | Comment |
---|---|---|---|
Comparative tracking index | 150 V Show Supplier Material materials with Comparative tracking index of 150 V | IEC 60112 | Sol.A |
Rheological Properties
Property | Value | Testing Standard | Condition | Comment |
---|---|---|---|---|
Melt mass-flow rate | 40 g/10min Show Supplier Material materials with Melt mass-flow rate of 40 g/10min | ISO 1133 | 315°C/5Kg | |
Shrinkage | 0.2 % Show Supplier Material materials with Shrinkage of 0.2 % | ISO 294-4 | 330/140/50* | *Melt Temp. [°C] / Mold Temp. [°C] / Cavity Press. [MPa] |
0.6 % Show Supplier Material materials with Shrinkage of 0.6 % | ISO 294-4 | 330/140/50* | *Melt Temp. [°C] / Mold Temp. [°C] / Cavity Press. [MPa], Transverse |
Technological properties
Property | ||
---|---|---|
Additives | Release agent | |
Certifications | RoHS 2011/65/UE | |
Color | Natural | |
Features | Flame Retardant, Impact Modified, Heat Stabilized | |
Fillers | 40% Glass Fiber | |
Processing methods | Injection Molding |