General
Property | Temperature | Value | Testing Standard | Condition | Thickness | Comment |
---|---|---|---|---|---|---|
Density | 1.68 g/cm³ Show Supplier Material materials with Density of 1.68 g/cm³ | ISO 1183 | ||||
Moisture absorption | 23 °C | 0.1 % Show Supplier Material materials with Moisture absorption of 0.1 % | ISO 62 | 50%RH | 2 mm | |
Water absorption | 0.3 % Show Supplier Material materials with Water absorption of 0.3 % | ISO 62 | 2 mm | immersion at 23°C |
Mechanical
Property | Temperature | Value | Testing Standard | Comment |
---|---|---|---|---|
Elastic modulus | 3.6 GPa Show Supplier Material materials with Elastic modulus of 3.6 GPa | ISO 527-2/1A | 1mm/min | |
Elongation | 8.5 % Show Supplier Material materials with Elongation of 8.5 % | ISO 527-2/1A | 50mm/min | nominal | |
Elongation at yield | 2.8 % Show Supplier Material materials with Elongation at yield of 2.8 % | ISO 527-2/1A | 50mm/min | |
Flexural modulus | 3.6 GPa Show Supplier Material materials with Flexural modulus of 3.6 GPa | ISO 178 | 2mm/min | |
Flexural strength | 85 MPa Show Supplier Material materials with Flexural strength of 85 MPa | ISO 178 | 2mm/min | |
Impact strength, Charpy notched | 23 °C | 3 kJ/m² Show Supplier Material materials with Impact strength, Charpy notched of 3 kJ/m² | ISO 179/1eA | |
Impact strength, Charpy unnotched | 23 °C | 37 kJ/m² Show Supplier Material materials with Impact strength, Charpy unnotched of 37 kJ/m² | ISO 179/1eU | |
Yield strength | 53 MPa Show Supplier Material materials with Yield strength of 53 MPa | ISO 527-2/1A | 50mm/min |
Thermal
Property | Value | Testing Standard | Comment |
---|---|---|---|
Melting point | 225 °C Show Supplier Material materials with Melting point of 225 °C | ISO 11357-1/-3 | 10°C/min |
Rheological Properties
Property | Value | Testing Standard | Comment |
---|---|---|---|
Melt mass-flow rate | 20 g/10min Show Supplier Material materials with Melt mass-flow rate of 20 g/10min | ISO 1133 | 250°C/2.16Kg |
Technological properties
Property | ||
---|---|---|
Additives | Release agent | |
Certifications | Food Contact, RoHS 2011/65/UE | |
Color | Black | |
Features | Metal Detectable | |
Processing methods | Injection Molding |