General
Property | Value | Testing Standard |
---|---|---|
Density | 1.34 g/cm³ Show Supplier Material materials with Density of 1.34 g/cm³ | ISO 1183 |
Mechanical
Property | Temperature | Value | Testing Standard | Comment |
---|---|---|---|---|
Elastic modulus | 5.5 GPa Show Supplier Material materials with Elastic modulus of 5.5 GPa | ISO 527-2/1A | 1mm/min | |
Elongation | 3.4 % Show Supplier Material materials with Elongation of 3.4 % | ISO 527-2/1A | 5mm/min | |
Flexural modulus | 4.8 GPa Show Supplier Material materials with Flexural modulus of 4.8 GPa | ISO 178 | 2mm/min | |
Flexural strength | 150 MPa Show Supplier Material materials with Flexural strength of 150 MPa | ISO 178 | 2mm/min | |
Impact strength, Charpy notched | 23 °C | 7 kJ/m² Show Supplier Material materials with Impact strength, Charpy notched of 7 kJ/m² | ISO 179/1eA | |
Impact strength, Charpy unnotched | 23 °C | 55 kJ/m² Show Supplier Material materials with Impact strength, Charpy unnotched of 55 kJ/m² | ISO 179/1eU | |
Tensile strength | 100 MPa Show Supplier Material materials with Tensile strength of 100 MPa | ISO 527-2/1A | 5mm/min |
Thermal
Property | Value | Thickness | Testing Standard | Comment | |||
---|---|---|---|---|---|---|---|
Glow Wire Flammability Index | 700 °C Show Supplier Material materials with Glow Wire Flammability Index of 700 °C | 2 mm | IEC 60695-2-12 | ||||
Heat deflection temperature | 145 °C Show Supplier Material materials with Heat deflection temperature of 145 °C | ISO 75/2Af | 1.80 MPa | ||||
Melting point | 222 °C Show Supplier Material materials with Melting point of 222 °C | ISO 11357-1/-3 | 10°C/min | ||||
Flammability | Thickness tested (mm): 1.6, Class: HB, Standard: UL 94 |
Electrical
Property | Value | Testing Standard | Comment |
---|---|---|---|
Surface resistivity | 1e+10 Ω/sq Show Supplier Material materials with Surface resistivity of 1e+10 Ω/sq | IEC 60093 | 500V |
1e+12 Ω/sq Show Supplier Material materials with Surface resistivity of 1e+12 Ω/sq | IEC 60093 | 500V | |
Volume resistivity | 1e+11 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+11 Ω·cm | IEC 60093 | 500V |
1e+13 Ω·cm Show Supplier Material materials with Volume resistivity of 1e+13 Ω·cm | IEC 60093 | 500V |
Rheological Properties
Property | Value | Testing Standard | Condition | Comment |
---|---|---|---|---|
Melt mass-flow rate | 12 g/10min Show Supplier Material materials with Melt mass-flow rate of 12 g/10min | ISO 1133 | 250°C/2.16Kg | |
Shrinkage | 0.4 % Show Supplier Material materials with Shrinkage of 0.4 % | ISO 294-4 | 280/80/60* | *Melt Temp. [°C] / Mold Temp. [°C] / Cavity Press. [MPa] |
0.6 % Show Supplier Material materials with Shrinkage of 0.6 % | ISO 294-4 | 280/80/60* | *Melt Temp. [°C] / Mold Temp. [°C] / Cavity Press. [MPa], Transverse |
Technological properties
Property | ||
---|---|---|
Additives | Release agent | |
Certifications | RoHS 2011/65/UE | |
Color | Natural | |
Fillers | 15% Glass Fiber | |
Processing methods | Injection Molding |