General
Property | Temperature | Value | Condition | Testing Standard | Thickness | Comment |
---|---|---|---|---|---|---|
Density | 1.36 g/cm³ Show Supplier Material materials with Density of 1.36 g/cm³ | dry | ISO 1183 | |||
Moisture absorption | 23 °C | 1.6 % Show Supplier Material materials with Moisture absorption of 1.6 % | 50%RH | ISO 62 | 2 mm | |
Water absorption | 6.2 % Show Supplier Material materials with Water absorption of 6.2 % | ISO 62 | 2 mm | immersion at 23°C |
Mechanical
Property | Temperature | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|---|
Elastic modulus | 7.3 GPa Show Supplier Material materials with Elastic modulus of 7.3 GPa | 50%RH | ISO 527-2/1A | 1mm/min | |
9.7 GPa Show Supplier Material materials with Elastic modulus of 9.7 GPa | dry | ISO 527-2/1A | 1mm/min | ||
Elongation | 2.7 % Show Supplier Material materials with Elongation of 2.7 % | dry | ISO 527-2/1A | 5mm/min | |
4.5 % Show Supplier Material materials with Elongation of 4.5 % | 50%RH | ISO 527-2/1A | 5mm/min | ||
Flexural modulus | 9 GPa Show Supplier Material materials with Flexural modulus of 9 GPa | dry | ISO 178 | 2mm/min | |
Flexural strength | 235 MPa Show Supplier Material materials with Flexural strength of 235 MPa | dry | ISO 178 | 2mm/min | |
Impact strength, Charpy notched | 23 °C | 6 kJ/m² Show Supplier Material materials with Impact strength, Charpy notched of 6 kJ/m² | dry | ISO 179/1eA | |
23 °C | 10 kJ/m² Show Supplier Material materials with Impact strength, Charpy notched of 10 kJ/m² | 50%RH | ISO 179/1eA | ||
Impact strength, Charpy unnotched | 50 kJ/m² Show Supplier Material materials with Impact strength, Charpy unnotched of 50 kJ/m² | dry | ISO 179/1eU | 23°C | |
65 kJ/m² Show Supplier Material materials with Impact strength, Charpy unnotched of 65 kJ/m² | 50%RH | ISO 179/1eU | 23°C | ||
Tensile strength | 105 MPa Show Supplier Material materials with Tensile strength of 105 MPa | 50%RH | ISO 527-2/1A | 5mm/min | |
148 MPa Show Supplier Material materials with Tensile strength of 148 MPa | dry | ISO 527-2/1A | 5mm/min |
Thermal
Property | Value | Testing Standard | Comment |
---|---|---|---|
Melting point | 255 °C Show Supplier Material materials with Melting point of 255 °C | ISO 11357-1/-3 | 10°C/min |
Technological properties
Property | ||
---|---|---|
Additives | Release agent | |
Certifications | RoHS 2011/65/UE | |
Color | Black | |
Features | Hydrolysis Resistance, Heat Stabilized | |
Fillers | 30% Glass Fiber | |
Processing methods | Injection Molding |