General
Property | Value | Condition | Testing Standard |
---|---|---|---|
Density | 1.23 g/cm³ Show Supplier Material materials with Density of 1.23 g/cm³ | dry | ISO 1183 |
Mechanical
Property | Temperature | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|---|
Elastic modulus | 3.5 GPa Show Supplier Material materials with Elastic modulus of 3.5 GPa | 50%RH | ISO 527-2/1A | 1mm/min | |
6.0 GPa Show Supplier Material materials with Elastic modulus of 6.0 GPa | dry | ISO 527-2/1A | 1mm/min | ||
Elongation | 3 % Show Supplier Material materials with Elongation of 3 % | dry | ISO 527-2/1A | 5mm/min | |
12 % Show Supplier Material materials with Elongation of 12 % | 50%RH | ISO 527-2/1A | 5mm/min | ||
Flexural modulus | 2.7 GPa Show Supplier Material materials with Flexural modulus of 2.7 GPa | 50%RH | ISO 178 | 2mm/min | |
5.1 GPa Show Supplier Material materials with Flexural modulus of 5.1 GPa | dry | ISO 178 | 2mm/min | ||
Flexural strength | 125 MPa Show Supplier Material materials with Flexural strength of 125 MPa | 50%RH | ISO 178 | 2mm/min | |
205 MPa Show Supplier Material materials with Flexural strength of 205 MPa | dry | ISO 178 | 2mm/min | ||
Impact strength, Charpy notched | 23 °C | 5.5 kJ/m² Show Supplier Material materials with Impact strength, Charpy notched of 5.5 kJ/m² | dry | ISO 179/1eA | |
23 °C | 11 kJ/m² Show Supplier Material materials with Impact strength, Charpy notched of 11 kJ/m² | 50%RH | ISO 179/1eA | ||
Impact strength, Charpy unnotched | 45 kJ/m² Show Supplier Material materials with Impact strength, Charpy unnotched of 45 kJ/m² | dry | ISO 179/1eU | 23°C | |
65 kJ/m² Show Supplier Material materials with Impact strength, Charpy unnotched of 65 kJ/m² | 50%RH | ISO 179/1eU | 23°C | ||
Tensile strength | 70 MPa Show Supplier Material materials with Tensile strength of 70 MPa | 50%RH | ISO 527-2/1A | 5mm/min | |
126 MPa Show Supplier Material materials with Tensile strength of 126 MPa | dry | ISO 527-2/1A | 5mm/min |
Thermal
Property | Value | Testing Standard | Comment |
---|---|---|---|
Melting point | 218 °C Show Supplier Material materials with Melting point of 218 °C | ISO 11357-1/-3 | 10°C/min |
Rheological Properties
Property | Value | Testing Standard | Comment |
---|---|---|---|
Melt mass-flow rate | 28 g/10min Show Supplier Material materials with Melt mass-flow rate of 28 g/10min | ISO 1133 | 250°C/5Kg |
Technological properties
Property | ||
---|---|---|
Additives | Release agent | |
Certifications | RoHS 2011/65/UE | |
Color | Black | |
Features | Heat Stabilized | |
Fillers | 15% Glass Fiber | |
Processing methods | Injection Molding |