General
Property | Value | Condition | Testing Standard |
---|---|---|---|
Density | 1.1 g/cm³ Show Supplier Material materials with Density of 1.1 g/cm³ | dry | ISO 1183 |
Mechanical
Property | Temperature | Value | Condition | Testing Standard | Comment |
---|---|---|---|---|---|
Elastic modulus | 2.4 GPa Show Supplier Material materials with Elastic modulus of 2.4 GPa | dry | ISO 527-2/1A | 1mm/min | |
Flexural modulus | 2.3 GPa Show Supplier Material materials with Flexural modulus of 2.3 GPa | dry | ISO 178 | 2mm/min | |
Flexural strength | 82 MPa Show Supplier Material materials with Flexural strength of 82 MPa | dry | ISO 178 | 2mm/min | |
Impact strength, Charpy notched | -30 °C | 10.2 kJ/m² Show Supplier Material materials with Impact strength, Charpy notched of 10.2 kJ/m² | dry | ISO 179/1eA | |
23 °C | 17 kJ/m² Show Supplier Material materials with Impact strength, Charpy notched of 17 kJ/m² | dry | ISO 179/1eA | ||
Impact strength, Izod notched | 23 °C | 15 kJ/m² Show Supplier Material materials with Impact strength, Izod notched of 15 kJ/m² | dry | ISO 180/1A | |
Yield strength | 65 MPa Show Supplier Material materials with Yield strength of 65 MPa | dry | ISO 527-2/1A | 50mm/min |
Thermal
Property | Value | Testing Standard | Comment |
---|---|---|---|
Heat deflection temperature | 65 °C Show Supplier Material materials with Heat deflection temperature of 65 °C | ISO 75/2Af | 1.80 MPa |
190 °C Show Supplier Material materials with Heat deflection temperature of 190 °C | ISO 75/2Bf | 5mm | |
Melting point | 260 °C Show Supplier Material materials with Melting point of 260 °C | ISO 11357-1/-3 | 10°C/min |
Rheological Properties
Property | Value | Testing Standard | Comment |
---|---|---|---|
Melt mass-flow rate | 19 g/10min Show Supplier Material materials with Melt mass-flow rate of 19 g/10min | ISO 1133 | 275°C/2.16Kg |
Viscosity number | 140 cm³/gr Show Supplier Material materials with Viscosity number of 140 cm³/gr | ISO 307 | Sulfuric acid |
Technological properties
Property | ||
---|---|---|
Certifications | RoHS 2011/65/UE | |
Color | Black | |
Features | Impact Modified | |
Processing methods | Injection Molding |