Copolyamide 6I/6T (PA6I/6T)
RADILON AESTUS T1 RV300FC 306K BKGeliefert von:
RadiciGroup High Performance PolymersCopolyamide 6T/6I/66 (PA6T/6I/66)
RADILON AESTUS T1 RV300RKC 306 BKGeliefert von:
RadiciGroup High Performance PolymersPolybutylenterephthalat (PBT)
Crastin® SK695FR NC010Polyphthalamid (PPA)
Polyphthalamide Reinforced with 33% Glass Fibre (PPA+GF33)Geliefert von:
2 Matmatch-Lieferanten
Polyetheretherketon (PEEK)
Polyetheretherketone Reinforced with 30% Glass Fibre (PEEK+GF30)Geliefert von:
1 Matmatch-Lieferant
Polyamide 6 (PA6)
Polyamide 6 Reinforced with 50% Glass Fibers (PA6+GF50)Geliefert von:
2 Matmatch-Lieferanten
Polyamide 66 (PA66)
Polyamide 66 Reinforced with 50% Glass Fibers (PA66+GF50)Geliefert von:
4 Matmatch-Lieferanten
Polyesterharz (UP)
Unsaturated polyester Reinforced with 15% Glass Fibres and 55% Mineral Powder (UP+GF15+MD55),Type 802Polyesterharz (UP)
Unsaturated polyester Reinforced with 15% Glass Fibres and 60% Mineral Powder (UP+GF15+MD60), Type 804Polyamide 66 (PA66)
Polyamide 66 Reinforced with 30% Long Glass Fibers (PA66+LGF30)Geliefert von:
3 Matmatch-Lieferanten
Polyamide 46 (PA46)
Polyamide 46 Reinforced with 50% Glass Fibers (PA46+GF50)Geliefert von:
2 Matmatch-Lieferanten
Styrol-Acrylnitril (SAN)
Styrene acrylonitrile Reinforced with 35% Glass Fibre (SAN+GF35)Polyamide 46 (PA46)
Polyamide 46 Reinforced with 40% Glass Fibers (PA46+GF40)Geliefert von: