Cast Copper Bronze Aluminium Bronze
ASTM B505 Grade C95300 Heat-TreatedGeliefert von:
1 Matmatch-Lieferant
Cast Copper Bronze Aluminium Bronze
ASTM B505 Grade C95300 HT, Heat-TreatedGeliefert von:
1 Matmatch-Lieferant
Cast Copper Bronze Aluminium Bronze
ASTM B505 Grade C95500 Heat-TreatedGeliefert von:
1 Matmatch-Lieferant
Cast Copper Bronze Aluminium Bronze
ASTM B505 Grade C95500 HT, Heat-TreatedGeliefert von:
1 Matmatch-Lieferant
Austenitischer rostfreier Stahl
EN 10088-1 Grade X1CrNiMoN25-22-2 solution annealed (+AT)Austenitischer rostfreier Stahl
EN 10088-1 Grade X1CrNi25-21 solution annealed (+AT)Austenitischer rostfreier Stahl
EN 10028-7 Grade X1CrNi25-21 solution annealed (+AT)Austenitischer rostfreier Stahl
EN 10028-7 Grade X1CrNiMoN25-22-2 solution annealed (+AT)Austenitischer rostfreier Stahl
EN 10216-5 Grade X1CrNi25-21 solution annealed (+AT)Austenitischer rostfreier Stahl
EN 10216-5 Grade X1CrNiMoN25-22-2 solution annealed (+AT)Austenitischer rostfreier Stahl
EN 10025-5 Grade S355J2WP normalized or normalized formed (+N)Geliefert von:
1 Matmatch-Lieferant
Austenitischer rostfreier Stahl
EN 10095 Grade X15CrNiSi25-21 solution annealed (+AT)Austenitischer rostfreier Stahl
EN 10095 Grade X8CrNi25-21 solution annealed (+AT)Austenitischer rostfreier Stahl
SEW 470 Grade X8CrNi25-21 solution annealed (+AT)Austenitischer rostfreier Stahl
SEW 470 Grade X15CrNiSi25-21 solution annealed (+AT)