Módulo elástico: 110.3 - 122.7 GPa

Quick Comparison

Acero inoxidable austenítico

Sandvik 253 MA

Suministrada por:

Alleima (formerly Sandvik Materials Technology)

Bronce fosforado

UNS C52100 boway

Suministrada por:

Ningbo Boway Alloy Material

Wrought Copper Pure / Low Alloyed Copper

UNS C14415 boway

Suministrada por:

Ningbo Boway Alloy Material

Wrought Copper High Copper Alloy

ASTM B768 Grade C17510 TH04

Bronce fosforado

UNS C51100 boway

Suministrada por:

Ningbo Boway Alloy Material

Bronce fosforado

UNS C51000 boway

Suministrada por:

Ningbo Boway Alloy Material

Wrought Copper High Copper Alloy

UNS C19400 boway

Suministrada por:

Ningbo Boway Alloy Material

Wrought Copper High Copper Alloy

ASTM B768 Grade C17510 TF00

Nickel Chromium Iron Alloy

VDM® Alloy 718

Suministrada por:

VDM Metals

Acero inoxidable austenítico

Esshete 1250

Suministrada por:

Alleima (formerly Sandvik Materials Technology)

Wrought Copper High Copper Alloy

ASTM B251 Grade C17000 TD04

Wrought Copper High Copper Alloy

ASTM B196 Grade C17000 TF00

Wrought Copper High Copper Alloy

ASTM B196 Grade C17000 TB00

Wrought Copper High Copper Alloy

ASTM B196 Grade C17000 TH04

Nickel Chromium Molybdenum Alloy

VDM® Alloy 602 CA

Suministrada por:

VDM Metals

Nickel Chromium Iron Alloy

VDM® Alloy 800

Suministrada por:

VDM Metals

Nickel Chromium Iron Alloy

VDM® Alloy 800 H

Suministrada por:

VDM Metals

Nickel Chromium Iron Alloy

VDM® Alloy 800 HP

Suministrada por:

VDM Metals

Aleación alfa-beta

AMS 4919 Grade R54620