Módulo elástico: 6.87 GPa

Quick Comparison

Polyvinylidenefluoride (PVDF)

Kynar Flex® 3120-10

Suministrada por:

Arkema: High Performance Polymers

Polyamide 6 (PA6)

Polyamide 6 Reinforced with 30% Glass Fibre (PA6+GF30)

Suministrada por:

3 proveedores de Matmatch

Polyamide 66 (PA66)

Polyamide 66 Reinforced with 30% Glass Fibre (PA66+GF30)

Suministrada por:

4 proveedores de Matmatch

Polyamide 12 (PA12)

Polyamide 12 Reinforced with 30% Glass Fibre (PA12+GF30)

Suministrada por:

1 proveedor Matmatch

Polyamide 6 (PA6)

Polyamide 6 Reinforced with 30% Long Glass Fibers (PA6+LGF30)

Suministrada por:

3 proveedores de Matmatch

Tereftalato de polibutileno (PBT)

Poly(butylene terephthalate) Reinforced with 20% Glass Fibers (PBT+GF20)

Suministrada por:

4 proveedores de Matmatch

Polyamide 6/66 (PA6/66)

Copolyamide 6/66 Reinforced with 30% Glass Fibers (PA6/66+GF30)

Suministrada por:

1 proveedor Matmatch

Polietileno tereftalato (PET)

Polyethylene terephthalate Reinforced with 15% Glass Fibers (PET+GF15)

Suministrada por:

2 proveedores de Matmatch

Polyamide 11 (PA11)

Polyamide 11 Reinforced with 30% Glass Fibre (PA11+GF30)

Suministrada por:

1 proveedor Matmatch

Polyamide 610 (PA610)

Polyamide 610 Reinforced with 30% Glass Fibre (PA610+GF30)

Suministrada por:

2 proveedores de Matmatch

Página 1 de 2