Description

Polyamide 11 reinforced with 30% glass fiber. Polyamide produced from a renewable source.

This material data has been provided by M-Base.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyValue

Density

1.25 - 1.26 g/cm³

Show Material materials with Density of 1.25 - 1.26 g/cm³

Mechanical

PropertyValueComment

Elastic modulus

6.2 - 7.3 GPa

Show Material materials with Elastic modulus of 6.2 - 7.3 GPa

Elongation

4.0 - 6.0 %

Show Material materials with Elongation of 4.0 - 6.0 %

Impact strength, Charpy notched

11.0 - 24.0 kJ/m²

Show Material materials with Impact strength, Charpy notched of 11.0 - 24.0 kJ/m²

Impact strength, Charpy unnotched

74 kJ/m²

Show Material materials with Impact strength, Charpy unnotched of 74 kJ/m²

89 kJ/m²

Show Material materials with Impact strength, Charpy unnotched of 89 kJ/m²

Tensile strength

110.0 - 134.0 MPa

Show Material materials with Tensile strength of 110.0 - 134.0 MPa

at 4-6% strain

Thermal

PropertyValueComment

Coefficient of thermal expansion

5e-05 - 8e-05 1/K

Show Material materials with Coefficient of thermal expansion of 5e-05 - 8e-05 1/K

Max service temperature

150 °C

Show Material materials with Max service temperature of 150 °C

Short

80 °C

Show Material materials with Max service temperature of 80 °C

Long

Melting point

183.0 - 189.0 °C

Show Material materials with Melting point of 183.0 - 189.0 °C

Thermal conductivity

0.4 W/(m·K)

Show Material materials with Thermal conductivity of 0.4 W/(m·K)

Flammability

UL 94 HB

Electrical

PropertyValue

Electrical resistivity

700000000000 Ω·m

Show Material materials with Electrical resistivity of 700000000000 Ω·m

Optical

PropertyValue

Transparency

no

Technological properties

Property
Fillers

30% Glass Fiber

Other

You are viewing a generic polymer page, for more information please contact the suppliers or Matmatch, or use our Search under the following link to find more specific grades and formulations based on your application:

Polymer Advanced Search

Processing methods

Injection molding