Description

Copolyamide 6.6/6 with 30% glass fiber reinforced, heat stabilised, excellent UV stabilised, offers an excellent combination between impact resistance and rigidity. It is thermal resistance and surface appearance, good surface aspect.

This material data has been provided by M-Base.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyValue

Density

1.33 - 1.37 g/cm³

Show Material materials with Density of 1.33 - 1.37 g/cm³

Mechanical

PropertyValueComment

Elastic modulus

5.5 - 7.5 GPa

Show Material materials with Elastic modulus of 5.5 - 7.5 GPa

Elongation

5.0 - 8.0 %

Show Material materials with Elongation of 5.0 - 8.0 %

Impact strength, Charpy notched

10.0 - 25.0 kJ/m²

Show Material materials with Impact strength, Charpy notched of 10.0 - 25.0 kJ/m²

Impact strength, Charpy unnotched

80 kJ/m²

Show Material materials with Impact strength, Charpy unnotched of 80 kJ/m²

100 kJ/m²

Show Material materials with Impact strength, Charpy unnotched of 100 kJ/m²

Tensile strength

90.0 - 125.0 MPa

Show Material materials with Tensile strength of 90.0 - 125.0 MPa

at 5-8% strain

Thermal

PropertyValue

Coefficient of thermal expansion

2e-05 - 0.00011 1/K

Show Material materials with Coefficient of thermal expansion of 2e-05 - 0.00011 1/K

Melting point

240.0 - 260.0 °C

Show Material materials with Melting point of 240.0 - 260.0 °C

Flammability

UL 94 HB

Electrical

PropertyValue

Dielectric constant

4 [-]

Show Material materials with Dielectric constant of 4 [-]

9 [-]

Show Material materials with Dielectric constant of 9 [-]

Electrical resistivity

1000000000.0 - 10000000000000.0 Ω·m

Show Material materials with Electrical resistivity of 1000000000.0 - 10000000000000.0 Ω·m

Optical

PropertyValue

Transparency

no

Technological properties

Property
Application areas

Carbon brush holders, fuel tank caps, bumper support, oil filler pipes, radiatorcaps, gear wheels

Fillers

30% Glass Fiber

Other

You are viewing a generic polymer page, for more information please contact the suppliers or Matmatch, or use our Search under the following link to find more specific grades and formulations based on your application:

Polymer Advanced Search

Processing methods

Injection molding, extrusion, blow molding