Polycarbonate Reinforced with 30% Glass Fibers (PC+GF30)

Alternative and trade names
Makrolon®, Lexan®
Want to keep this datasheet? Save it now in your required format

Description

Reinforced poylcarbonate with 30% glass fiber.


  • High viscosity
  • Easy release extrusion
  • This material data has been provided by M-Base.

    All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
    Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

    Ashby charts

    See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

    Properties

    General

    PropertyValue

    Density

    1.35 - 1.46 g/cm³

    Show Material materials with Density of 1.35 - 1.46 g/cm³

    Mechanical

    PropertyValueComment

    Elastic modulus

    6.0 - 9.0 GPa

    Show Material materials with Elastic modulus of 6.0 - 9.0 GPa

    Elongation

    1.0 - 3.5 %

    Show Material materials with Elongation of 1.0 - 3.5 %

    Impact strength, Charpy notched

    4.0 - 17.0 kJ/m²

    Show Material materials with Impact strength, Charpy notched of 4.0 - 17.0 kJ/m²

    Impact strength, Charpy unnotched

    30 kJ/m²

    Show Material materials with Impact strength, Charpy unnotched of 30 kJ/m²

    60 kJ/m²

    Show Material materials with Impact strength, Charpy unnotched of 60 kJ/m²

    Tensile strength

    60.0 - 160.0 MPa

    Show Material materials with Tensile strength of 60.0 - 160.0 MPa

    at 1-3.5% strain

    Thermal

    PropertyValue

    Coefficient of thermal expansion

    2e-05 - 7e-05 1/K

    Show Material materials with Coefficient of thermal expansion of 2e-05 - 7e-05 1/K

    Specific heat capacity

    1100 J/(kg·K)

    Show Material materials with Specific heat capacity of 1100 J/(kg·K)

    Thermal conductivity

    0.24 W/(m·K)

    Show Material materials with Thermal conductivity of 0.24 W/(m·K)

    Flammability

    UL 94 V2-V0

    Electrical

    PropertyValue

    Dielectric constant

    3.1 [-]

    Show Material materials with Dielectric constant of 3.1 [-]

    3.6 [-]

    Show Material materials with Dielectric constant of 3.6 [-]

    Electrical resistivity

    10000000000000.0 - 100000000000000.0 Ω·m

    Show Material materials with Electrical resistivity of 10000000000000.0 - 100000000000000.0 Ω·m

    Optical

    PropertyValue

    Transparency

    no

    Technological properties

    Property
    Application areas

    Housing parts

    Fillers

    30% Glass Fiber

    Processing methods

    Injection molding