Conductividad térmica: 11.9 - 12 W/(m·K)

Quick Comparison

Acero inoxidable austenítico

Alloy 24 / 1.4565 Solution annealed and quenched

Suministrada por:

Hempel Special Metals

Superaustenitic Stainless Steel

Acidur 4529

Suministrada por:

Deutsche Edelstahlwerke (DEW)

Nickel Steel

ASTM A353 Double-Normalized and Tempered

Suministrada por:

1 proveedor Matmatch

Acero inoxidable austenítico

Sanicro® 25

Suministrada por:

Alleima (formerly Sandvik Materials Technology)

Superaustenitic Stainless Steel

VDM® Alloy 926

Suministrada por:

VDM Metals

Nickel Chromium Iron Alloy

Sanicro 31HT

Suministrada por:

Alleima (formerly Sandvik Materials Technology)

Tin Bronze

ASTM B505 Grade C90700

Suministrada por:

1 proveedor Matmatch

Leaded Tin Bronze

ASTM B505 Grade C92700

Suministrada por:

1 proveedor Matmatch

Cast Copper Bronze Aluminium Bronze

ASTM B505 Grade C95200

Suministrada por:

1 proveedor Matmatch

Cast Copper Bronze Aluminium Bronze

ASTM B505 Grade C95300 Heat-Treated

Suministrada por:

1 proveedor Matmatch

Cast Copper Bronze Aluminium Bronze

ASTM B505 Grade C95300 HT, Heat-Treated

Suministrada por:

1 proveedor Matmatch

Cast Copper Bronze Aluminium Bronze

ASTM B505 Grade C95500 Heat-Treated

Suministrada por:

1 proveedor Matmatch

Cast Copper Bronze Aluminium Bronze

ASTM B505 Grade C95500 HT, Heat-Treated

Suministrada por:

1 proveedor Matmatch

Cast Copper Bronze Aluminium Bronze

ASTM B505 Grade C95520

Suministrada por:

1 proveedor Matmatch

Nickel Chromium Iron Alloy

Sandvik 2RK65™

Suministrada por:

Alleima (formerly Sandvik Materials Technology)

Superaustenitic Stainless Steel

1.4529 / X1NiCrMoCuN25-20-7

Suministrada por:

HSM Stahl- und Metallhandel GmbH

Acero inoxidable austenítico

UGI® 202N – Grade 1 Annealed

Suministrada por:

Ugitech
Página 1 de 118