Acero inoxidable austenítico
Sandvik 253 MASuministrada por:
Alleima (formerly Sandvik Materials Technology)Nickel Chromium Iron Alloy
Sanicro® 28Suministrada por:
Alleima (formerly Sandvik Materials Technology)Medium Carbon Steel
EN 10083-3 Grade 30MnB5 quenched and tempered (+QT)Suministrada por:
1 proveedor Matmatch
Acero inoxidable austenítico
Esshete 1250Suministrada por:
Alleima (formerly Sandvik Materials Technology)Acero inoxidable martensítico
ASTM A841 Grade A Class 1 Thermo-Mechanical Control Process (TMCP)Suministrada por:
1 proveedor Matmatch
Acero inoxidable austenítico
Sanicro® 25Suministrada por:
Alleima (formerly Sandvik Materials Technology)Acero inoxidable ferrítico
Sandvik 4C54Suministrada por:
Alleima (formerly Sandvik Materials Technology)