Printdur® 2343

Alternative and trade names
1.2343
Want to keep this datasheet? Save it now in your required format

Description

1.2343 is a tool steel used for 3D printing (additive manufacturing) purposes.

Equivalent Materials

This material data has been provided by Deutsche Edelstahlwerke Specialty Steel (DEW).

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

Chemical properties

PropertyValue

Carbon

0.37 %

Show Supplier Material materials with Carbon of 0.37 %

Chromium

5.5 %

Show Supplier Material materials with Chromium of 5.5 %

Iron

Balance

Manganese

0.5 %

Show Supplier Material materials with Manganese of 0.5 %

Molybdenum

1.3 %

Show Supplier Material materials with Molybdenum of 1.3 %

Silicon

1 %

Show Supplier Material materials with Silicon of 1 %

Vanadium

0.4 %

Show Supplier Material materials with Vanadium of 0.4 %

Technological properties

Property
Application areas

Additive manufacturing