Rapidur PM-M4

Alternative and trade names
DIN EN ISO HS6-5-4, 1.3351, AISI M4
Want to keep this datasheet? Save it now in your required format

Description

1.3351 (HS6-5-4) high speed tool steel with increased C & V content and volume fraction for higher wear resistance.

Equivalent Materials

This material data has been provided by Deutsche Edelstahlwerke Specialty Steel (DEW).

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyValue

Density

7.9 g/cm³

Show Supplier Material materials with Density of 7.9 g/cm³

Mechanical

PropertyValue

Elastic modulus

230 GPa

Show Supplier Material materials with Elastic modulus of 230 GPa

Hardness, Rockwell C

59.0 - 65.0 [-]

Show Supplier Material materials with Hardness, Rockwell C of 59.0 - 65.0 [-]

Thermal

PropertyTemperatureValue

Specific heat capacity

430.0 J/(kg·K)

Show Supplier Material materials with Specific heat capacity of 430.0 J/(kg·K)

Thermal conductivity

20 °C

22 W/(m·K)

Show Supplier Material materials with Thermal conductivity of 22 W/(m·K)

Electrical

PropertyValue

Electrical resistivity

5.3e-07 Ω·m

Show Supplier Material materials with Electrical resistivity of 5.3e-07 Ω·m

Chemical properties

PropertyValue

Carbon

1.35

Show Supplier Material materials with Carbon of 1.35

Chromium

4.1

Show Supplier Material materials with Chromium of 4.1

Molybdenum

5.0

Show Supplier Material materials with Molybdenum of 5.0

Tungsten

6.0

Show Supplier Material materials with Tungsten of 6.0

Vanadium

4.1

Show Supplier Material materials with Vanadium of 4.1

Technological properties

Property
Application areas

Thread-cutting tools, reamers, heavy-duty milling cutters, drills, punching tools