Temperatura de fusión: 860 °C

Quick Comparison

Tin Bronze

ASTM B505 Grade C90700

Suministrada por:

1 proveedor Matmatch

Leaded Tin Bronze

ASTM B505 Grade C92700

Suministrada por:

1 proveedor Matmatch

Cast Copper Bronze Aluminium Bronze

ASTM B505 Grade C95200

Suministrada por:

1 proveedor Matmatch

Cast Copper Bronze Aluminium Bronze

ASTM B505 Grade C95300 Heat-Treated

Suministrada por:

1 proveedor Matmatch

Cast Copper Bronze Aluminium Bronze

ASTM B505 Grade C95300 HT, Heat-Treated

Suministrada por:

1 proveedor Matmatch

Cast Copper Bronze Aluminium Bronze

ASTM B505 Grade C95500 Heat-Treated

Suministrada por:

1 proveedor Matmatch

Cast Copper Bronze Aluminium Bronze

ASTM B505 Grade C95500 HT, Heat-Treated

Suministrada por:

1 proveedor Matmatch

Cast Copper Bronze Aluminium Bronze

ASTM B505 Grade C95520

Suministrada por:

1 proveedor Matmatch

Bronce fosforado

JIS C5240HQ Harada

Suministrada por:

HARADA METAL INDUSTRY CO., LTD.

Bronce fosforado

JIS C5240 Harada

Suministrada por:

HARADA METAL INDUSTRY CO., LTD.

Wrought Copper High Copper Alloy

EN 1652 Grade CuCo2Be TH

Wrought Copper High Copper Alloy

EN 1652 Grade CuBe2 TH

Wrought Copper Nickel Silver Grade

SILVERSPEED-XL Nickel Silver

Wrought Copper High Copper Alloy

EN 1652 Grade CuNi2Be TH

Wrought Copper High Copper Alloy

EN 12164 Grade CuPb1P R250

Wrought Copper High Copper Alloy

EN 12164 Grade CuPb1P R300

Wrought Copper High Copper Alloy

EN 12163 Grade CuCo2Be R730

Wrought Copper High Copper Alloy

EN 12163 Grade CuCo2Be R680

Wrought Copper High Copper Alloy

EN 12167 Grade CuCo2Be R730