Formadur 2083 Superclean Plate

Alternative and trade names
DIN EN ISO X40Cr14, AISI 420, 1.2083, AFNOR Z40C14
Want to keep this datasheet? Save it now in your required format

Description

1.2083 (X40Cr14) Quenched and Tempered steel plate exhibits good corrosion-resistant and excellent polishability.

Equivalent Materials

This material data has been provided by Deutsche Edelstahlwerke Specialty Steel (DEW).

"Typical" values were obtained via a literature search. "Predicted" values were imputed via artificial intelligence technology. While we have placed significant efforts in ensuring data accuracy, "typical" and "predicted" data should be considered indicative and verified by appropriate material testing. Please do contact us if additional information on the the predicted data method is required.
All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

Dimension

PropertyValueThickness

Thickness

40.0 mm

Show Supplier Material materials with Thickness of 40.0 mm

40.0 mm

350.0 mm

Show Supplier Material materials with Thickness of 350.0 mm

350.0 mm

Width

900.0 mm

Show Supplier Material materials with Width of 900.0 mm

1100.0 mm

Show Supplier Material materials with Width of 1100.0 mm

Mechanical

PropertyValueComment

Hardness, Brinell

230.0

Show Supplier Material materials with Hardness, Brinell of 230.0

soft annealed

Hardness, Rockwell C

48.0 - 56.0 [-]

Show Supplier Material materials with Hardness, Rockwell C of 48.0 - 56.0 [-]

Tensile strength

1555.0 - 1775.0 MPa

Show Supplier Material materials with Tensile strength of 1555.0 - 1775.0 MPa

Thermal

PropertyTemperatureValueComment

Coefficient of thermal expansion

100 °C

0.0000111 1/K

Show Supplier Material materials with Coefficient of thermal expansion of 0.0000111 1/K

for 20°C to the mentioned temperature

150 °C

0.0000113 1/K

Show Supplier Material materials with Coefficient of thermal expansion of 0.0000113 1/K

for 20°C to the mentioned temperature

200 °C

0.0000116 1/K

Show Supplier Material materials with Coefficient of thermal expansion of 0.0000116 1/K

for 20°C to the mentioned temperature

250 °C

0.0000118 1/K

Show Supplier Material materials with Coefficient of thermal expansion of 0.0000118 1/K

for 20°C to the mentioned temperature

300 °C

0.000012 1/K

Show Supplier Material materials with Coefficient of thermal expansion of 0.000012 1/K

for 20°C to the mentioned temperature

350 °C

0.0000123 1/K

Show Supplier Material materials with Coefficient of thermal expansion of 0.0000123 1/K

for 20°C to the mentioned temperature

400 °C

0.0000124 1/K

Show Supplier Material materials with Coefficient of thermal expansion of 0.0000124 1/K

for 20°C to the mentioned temperature

450 °C

0.0000125 1/K

Show Supplier Material materials with Coefficient of thermal expansion of 0.0000125 1/K

for 20°C to the mentioned temperature

500 °C

0.0000126 1/K

Show Supplier Material materials with Coefficient of thermal expansion of 0.0000126 1/K

for 20°C to the mentioned temperature

Thermal conductivity

23 °C

22.6 W/(m·K)

Show Supplier Material materials with Thermal conductivity of 22.6 W/(m·K)

150 °C

24 W/(m·K)

Show Supplier Material materials with Thermal conductivity of 24 W/(m·K)

300 °C

24.6 W/(m·K)

Show Supplier Material materials with Thermal conductivity of 24.6 W/(m·K)

350 °C

24.9 W/(m·K)

Show Supplier Material materials with Thermal conductivity of 24.9 W/(m·K)

400 °C

24.4 W/(m·K)

Show Supplier Material materials with Thermal conductivity of 24.4 W/(m·K)

500 °C

23.7 W/(m·K)

Show Supplier Material materials with Thermal conductivity of 23.7 W/(m·K)

Chemical properties

PropertyValue

Carbon

0.4

Show Supplier Material materials with Carbon of 0.4

Chromium

13.5

Show Supplier Material materials with Chromium of 13.5

Manganese

0.9

Show Supplier Material materials with Manganese of 0.9

Silicon

0.35000000000000003

Show Supplier Material materials with Silicon of 0.35000000000000003

Technological properties

Property
Application areas

Moulds and inserts for processing corrosive acting plastics.

Heat Treatment

Soft annealing: 760-800°C (Cooling in furnace) - Hardening: 1000-1050°C and quenching in air, oil or hot bath T=500-550°C