Formadur 2085 Plate

Alternative and trade names
DIN EN ISO X33CrS16, AISI 420FM, 1.2085,
Want to keep this datasheet? Save it now in your required format

Description

1.2085 (X33CrS16) Quenched and Tempered steel plate suitable for mould frames, plastic moulds without special demands on surface quality.

Equivalent Materials

This material data has been provided by Deutsche Edelstahlwerke Specialty Steel (DEW).

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

Dimension

PropertyValueThickness

Thickness

15.0 mm

Show Supplier Material materials with Thickness of 15.0 mm

15.0 mm

225.0 mm

Show Supplier Material materials with Thickness of 225.0 mm

225.0 mm

Width

700.0 mm

Show Supplier Material materials with Width of 700.0 mm

1010.0 mm

Show Supplier Material materials with Width of 1010.0 mm

Mechanical

PropertyValueComment

Hardness, Brinell

280.0 - 325.0 [-]

Show Supplier Material materials with Hardness, Brinell of 280.0 - 325.0 [-]

as-delivered condition

Hardness, Rockwell C

30.0 - 48.0 [-]

Show Supplier Material materials with Hardness, Rockwell C of 30.0 - 48.0 [-]

Tensile strength

950.0 - 1095.0 MPa

Show Supplier Material materials with Tensile strength of 950.0 - 1095.0 MPa

Chemical properties

PropertyValue

Carbon

0.33

Show Supplier Material materials with Carbon of 0.33

Chromium

16.0

Show Supplier Material materials with Chromium of 16.0

Manganese

1.2

Show Supplier Material materials with Manganese of 1.2

Nickel

0.5

Show Supplier Material materials with Nickel of 0.5

Silicon

0.30000000000000004

Show Supplier Material materials with Silicon of 0.30000000000000004

Sulfur

0.05

Show Supplier Material materials with Sulfur of 0.05

Technological properties

Property
Application areas

Mould frames, plastic moulds without special demands on surface quality.

Heat Treatment

Soft annealing: 850-880°C (Cooling in furnace) - Hardening: 1000-1050°C and quenching in oil