Dimension
Property | Value |
---|---|
Thickness | 85 - 500 mm Show Supplier Material materials with Thickness of 85 - 500 mm |
Width | 850 - 900 mm Show Supplier Material materials with Width of 850 - 900 mm |
Mechanical
Property | Value | Temperature | Comment |
---|---|---|---|
Hardness, Brinell | 235 [-] Show Supplier Material materials with Hardness, Brinell of 235 [-] at 23.0 °C | 23.0 °C | soft annealed |
Hardness, Rockwell C | 42 - 52 [-] Show Supplier Material materials with Hardness, Rockwell C of 42 - 52 [-] at 23.0 °C | 23.0 °C | |
Tensile strength | 1320 - 1775 MPa Show Supplier Material materials with Tensile strength of 1320 - 1775 MPa at 23.0 °C | 23.0 °C |
Thermal
Property | Value | Temperature | Comment |
---|---|---|---|
Coefficient of thermal expansion | 1.19E-5 1/K Show Supplier Material materials with Coefficient of thermal expansion of 1.19E-5 1/K at 100.0 °C | 100.0 °C | for 20°C to the mentioned temperature |
1.25E-5 1/K Show Supplier Material materials with Coefficient of thermal expansion of 1.25E-5 1/K at 200.0 °C | 200.0 °C | for 20°C to the mentioned temperature | |
1.26E-5 1/K Show Supplier Material materials with Coefficient of thermal expansion of 1.26E-5 1/K at 300.0 °C | 300.0 °C | for 20°C to the mentioned temperature | |
1.28E-5 1/K Show Supplier Material materials with Coefficient of thermal expansion of 1.28E-5 1/K at 400.0 °C | 400.0 °C | for 20°C to the mentioned temperature | |
1.31E-5 1/K Show Supplier Material materials with Coefficient of thermal expansion of 1.31E-5 1/K at 500.0 °C | 500.0 °C | for 20°C to the mentioned temperature | |
1.33E-5 1/K Show Supplier Material materials with Coefficient of thermal expansion of 1.33E-5 1/K at 600.0 °C | 600.0 °C | for 20°C to the mentioned temperature | |
1.35E-5 1/K Show Supplier Material materials with Coefficient of thermal expansion of 1.35E-5 1/K at 700.0 °C | 700.0 °C | for 20°C to the mentioned temperature | |
Thermal conductivity | 29.8 W/(m·K) Show Supplier Material materials with Thermal conductivity of 29.8 W/(m·K) at 20.0 °C | 20.0 °C | |
33.9 W/(m·K) Show Supplier Material materials with Thermal conductivity of 33.9 W/(m·K) at 350.0 °C | 350.0 °C | ||
35.3 W/(m·K) Show Supplier Material materials with Thermal conductivity of 35.3 W/(m·K) at 700.0 °C | 700.0 °C | ||
Chemical properties
Property | ||
---|---|---|
Carbon | 0.37 % | |
Chromium | 5 % | |
Iron | Balance | |
Manganese | 0.4 % | |
Silicon | 0.3 % | |
Vanadium | 0.6 % |
Technological properties
Property | ||
---|---|---|
Application areas | As Thermodur 2367 EFS for your most challenging requirements | |
Heat Treatment | Soft annealing: 730-880°C (Cooling in furnace) - Hardening: 1020-1050°C and quenching in air, oil or hot bath T=500-550°C |