Cryodur 2249

Alternative and trade names
DIN EN ISO 45SiCrV6, 1.2249
Want to keep this datasheet? Save it now in your required format

Description

1.2249 (45SiCrV6) Quenched and Tempered cold work tool steel bar with good toughness and impact resistance.

Equivalent Materials

This material data has been provided by Deutsche Edelstahlwerke Specialty Steel (DEW).

"Typical" values were obtained via a literature search. "Predicted" values were imputed via artificial intelligence technology. While we have placed significant efforts in ensuring data accuracy, "typical" and "predicted" data should be considered indicative and verified by appropriate material testing. Please do contact us if additional information on the the predicted data method is required.
All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

Mechanical

PropertyValueComment

Hardness, Brinell

219 [-]

Show Supplier Material materials with Hardness, Brinell of 219 [-]

soft annealed

Hardness, Rockwell C

50 - 57 [-]

Show Supplier Material materials with Hardness, Rockwell C of 50 - 57 [-]

Tensile strength

1665 - 2105 MPa

Show Supplier Material materials with Tensile strength of 1665 - 2105 MPa

Chemical properties

PropertyValue

Carbon

0.45 %

Show Supplier Material materials with Carbon of 0.45 %

Chromium

1.35 %

Show Supplier Material materials with Chromium of 1.35 %

Iron

Balance

Manganese

0.65 %

Show Supplier Material materials with Manganese of 0.65 %

Silicon

1.35 %

Show Supplier Material materials with Silicon of 1.35 %

Vanadium

0.1 %

Show Supplier Material materials with Vanadium of 0.1 %

Technological properties

Property
Application areas

Pneumatic chipping hammers, punching tools, riveting hammers, punches and woodworking tools

Heat Treatment

Soft annealing: 710-740°C (Cooling in furnace) - Stress-relief-annealing: 650-680°C, Hardening: 860-890°C and quenching in oil