Cryodur 2363 Bar

Alternative and trade names
DIN EN ISO X100CrMoV5, 1.2363,AISI A2,AFNOR Z100CDV5
Want to keep this datasheet? Save it now in your required format

Description

1.2363 (X100CrMoV5) Quenched and Tempered cold work tool steel bar with high dimensional stability during heat treatment and high wear resistance and toughness.

Equivalent Materials

This material data has been provided by Deutsche Edelstahlwerke Specialty Steel (DEW).

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

Dimension

PropertyValue

Diameter

20.5 mm

Show Supplier Material materials with Diameter of 20.5 mm

353.0 mm

Show Supplier Material materials with Diameter of 353.0 mm

Mechanical

PropertyValueComment

Hardness, Brinell

231.0

Show Supplier Material materials with Hardness, Brinell of 231.0

soft annealed

Hardness, Rockwell C

56.0 - 62.0 [-]

Show Supplier Material materials with Hardness, Rockwell C of 56.0 - 62.0 [-]

Thermal

PropertyTemperatureValue

Thermal conductivity

100 °C

15.8 W/(m·K)

Show Supplier Material materials with Thermal conductivity of 15.8 W/(m·K)

350 °C

26.7 W/(m·K)

Show Supplier Material materials with Thermal conductivity of 26.7 W/(m·K)

700 °C

29.1 W/(m·K)

Show Supplier Material materials with Thermal conductivity of 29.1 W/(m·K)

Chemical properties

PropertyValue

Carbon

1.0

Show Supplier Material materials with Carbon of 1.0

Chromium

5.0

Show Supplier Material materials with Chromium of 5.0

Manganese

0.5

Show Supplier Material materials with Manganese of 0.5

Molybdenum

0.9500000000000001

Show Supplier Material materials with Molybdenum of 0.9500000000000001

Silicon

0.30000000000000004

Show Supplier Material materials with Silicon of 0.30000000000000004

Vanadium

0.2

Show Supplier Material materials with Vanadium of 0.2

Technological properties

Property
Application areas

Cutting tools, rolls, shear blades, cold pilger mandrels, cold stamping tools, plastic moulds

Heat Treatment

Soft annealing: 610-650°C (Cooling in furnace) - Stress-relief-annealing: 600°C (cooling in Furnace), Hardening: 930-970°C and quenching in oil, air or salt bath: 500-550°C