Cryodur 2826 Bar

Alternative and trade names
DIN EN ISO 60MnSiCr4, 1.2826, AISI S6
Want to keep this datasheet? Save it now in your required format

Description

1.2826 (60MnSiCr4) Quenched and Tempered steel bar with high toughness and good resilience in tempered condition.

Equivalent Materials

This material data has been provided by Deutsche Edelstahlwerke Specialty Steel (DEW).

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

Dimension

PropertyValue

Diameter

10.0 mm

Show Supplier Material materials with Diameter of 10.0 mm

220.0 mm

Show Supplier Material materials with Diameter of 220.0 mm

Mechanical

PropertyValueComment

Hardness, Brinell

220.0

Show Supplier Material materials with Hardness, Brinell of 220.0

soft annealed

Hardness, Rockwell C

51.0 - 59.0 [-]

Show Supplier Material materials with Hardness, Rockwell C of 51.0 - 59.0 [-]

Chemical properties

PropertyValue

Carbon

0.63

Show Supplier Material materials with Carbon of 0.63

Chromium

0.30000000000000004

Show Supplier Material materials with Chromium of 0.30000000000000004

Manganese

1.1

Show Supplier Material materials with Manganese of 1.1

Silicon

0.8

Show Supplier Material materials with Silicon of 0.8

Technological properties

Property
Application areas

Special steel for spring collets

Heat Treatment

Soft annealing: 680-720°C (Cooling in furnace) - Stress-relief-annealing: 650°C (cooling in Furnace), Hardening: 820-860°C and quenching in air, oil or salt bath: 180-220°C