Formadur 400 Plate

Want to keep this datasheet? Save it now in your required format

Description

Formadur 400 shows the following features and properties:


  • Pre-hardened plastic mold steel with approx. 400HB
  • Excellent toughness & hardenability
  • Excellent polishability (ESR)
  • Easy machinability
  • Good weldability
  • Best texturing properties
  • This material data has been provided by Deutsche Edelstahlwerke Specialty Steel (DEW).

    All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
    Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

    Ashby charts

    Properties

    Dimension

    PropertyValueThickness

    Thickness

    120.0 mm

    Show Supplier Material materials with Thickness of 120.0 mm

    120.0 mm

    600.0 mm

    Show Supplier Material materials with Thickness of 600.0 mm

    600.0 mm

    Width

    950.0 mm

    Show Supplier Material materials with Width of 950.0 mm

    1100.0 mm

    Show Supplier Material materials with Width of 1100.0 mm

    Mechanical

    PropertyValueComment

    Hardness, Brinell

    365.0 - 410.0 [-]

    Show Supplier Material materials with Hardness, Brinell of 365.0 - 410.0 [-]

    as-delivered condition

    Hardness, Rockwell C

    28.0 - 51.0 [-]

    Show Supplier Material materials with Hardness, Rockwell C of 28.0 - 51.0 [-]

    Tensile strength

    1220.0 - 1385.0 MPa

    Show Supplier Material materials with Tensile strength of 1220.0 - 1385.0 MPa

    Thermal

    PropertyTemperatureValueComment

    Coefficient of thermal expansion

    100 °C

    0.0000111 1/K

    Show Supplier Material materials with Coefficient of thermal expansion of 0.0000111 1/K

    for 20°C to the mentioned temperature

    200 °C

    0.0000129 1/K

    Show Supplier Material materials with Coefficient of thermal expansion of 0.0000129 1/K

    for 20°C to the mentioned temperature

    300 °C

    0.0000134 1/K

    Show Supplier Material materials with Coefficient of thermal expansion of 0.0000134 1/K

    for 20°C to the mentioned temperature

    400 °C

    0.0000135 1/K

    Show Supplier Material materials with Coefficient of thermal expansion of 0.0000135 1/K

    for 20°C to the mentioned temperature

    500 °C

    0.0000138 1/K

    Show Supplier Material materials with Coefficient of thermal expansion of 0.0000138 1/K

    for 20°C to the mentioned temperature

    600 °C

    0.0000141 1/K

    Show Supplier Material materials with Coefficient of thermal expansion of 0.0000141 1/K

    for 20°C to the mentioned temperature

    700 °C

    0.0000143 1/K

    Show Supplier Material materials with Coefficient of thermal expansion of 0.0000143 1/K

    for 20°C to the mentioned temperature

    Thermal conductivity

    23 °C

    36 W/(m·K)

    Show Supplier Material materials with Thermal conductivity of 36 W/(m·K)

    150 °C

    37.4 W/(m·K)

    Show Supplier Material materials with Thermal conductivity of 37.4 W/(m·K)

    300 °C

    33 W/(m·K)

    Show Supplier Material materials with Thermal conductivity of 33 W/(m·K)

    Chemical properties

    PropertyValue

    Carbon

    0.36

    Show Supplier Material materials with Carbon of 0.36

    Chromium

    1.9

    Show Supplier Material materials with Chromium of 1.9

    Manganese

    0.9

    Show Supplier Material materials with Manganese of 0.9

    Molybdenum

    0.5

    Show Supplier Material materials with Molybdenum of 0.5

    Nickel

    0.5

    Show Supplier Material materials with Nickel of 0.5

    Silicon

    0.4

    Show Supplier Material materials with Silicon of 0.4

    Technological properties

    Property
    Application areas

    Plastic injection and extrusion moulds for all dimensions and deep engraving with high demands on polishability, wear resistance and core strength.

    Heat Treatment

    Soft annealing: 710-740°C (Cooling in furnace) - Hardening: 820-850°C and quenching in oil or polymer