Cryodur PM-V10

Want to keep this datasheet? Save it now in your required format

Description

Cryodur PM-V10 is a powder metallorgical cold work tool steel. It exhibits a high hardness and wear resistance with an adequate toughness. Microstructure consists of fine and homogeneous distributed vanadium rich monocarbides without segregations due to the powder metallurgical processing.

This material data has been provided by Deutsche Edelstahlwerke Specialty Steel (DEW).

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyValue

Density

7.4 g/cm³

Show Supplier Material materials with Density of 7.4 g/cm³

Mechanical

PropertyValue

Elastic modulus

220 GPa

Show Supplier Material materials with Elastic modulus of 220 GPa

Hardness, Rockwell C

59.0 - 62.0 [-]

Show Supplier Material materials with Hardness, Rockwell C of 59.0 - 62.0 [-]

Thermal

PropertyTemperatureValueComment

Coefficient of thermal expansion

100 °C

0.000011 1/K

Show Supplier Material materials with Coefficient of thermal expansion of 0.000011 1/K

for 20°C to the mentioned temperature

200 °C

0.0000111 1/K

Show Supplier Material materials with Coefficient of thermal expansion of 0.0000111 1/K

for 20°C to the mentioned temperature

300 °C

0.0000113 1/K

Show Supplier Material materials with Coefficient of thermal expansion of 0.0000113 1/K

for 20°C to the mentioned temperature

400 °C

0.0000115 1/K

Show Supplier Material materials with Coefficient of thermal expansion of 0.0000115 1/K

for 20°C to the mentioned temperature

Chemical properties

PropertyValue

Carbon

2.45

Show Supplier Material materials with Carbon of 2.45

Chromium

5.3

Show Supplier Material materials with Chromium of 5.3

Manganese

0.5

Show Supplier Material materials with Manganese of 0.5

Molybdenum

1.3

Show Supplier Material materials with Molybdenum of 1.3

Silicon

0.9

Show Supplier Material materials with Silicon of 0.9

Sulfur

0.05

Show Supplier Material materials with Sulfur of 0.05

Vanadium

10.0

Show Supplier Material materials with Vanadium of 10.0

Technological properties

Property
Application areas

Various applications for cold work: punches, bending dies, cold forming presses, cutting knifes, screw conveyors