General
Property | Value | Temperature |
---|---|---|
Density | 8.1 g/cm³ Show Supplier Material materials with Density of 8.1 g/cm³ at 23.0 °C | 23.0 °C |
Mechanical
Property | Value | Temperature |
---|---|---|
Elastic modulus | 240 GPa Show Supplier Material materials with Elastic modulus of 240 GPa at 23.0 °C | 23.0 °C |
Hardness, Rockwell C | 60 - 68 [-] Show Supplier Material materials with Hardness, Rockwell C of 60 - 68 [-] at 23.0 °C | 23.0 °C |
Thermal
Property | Value | Temperature | Comment |
---|---|---|---|
Coefficient of thermal expansion | 1E-5 1/K Show Supplier Material materials with Coefficient of thermal expansion of 1E-5 1/K at 100.0 °C | 100.0 °C | for 20°C to the mentioned temperature |
1.05E-5 1/K Show Supplier Material materials with Coefficient of thermal expansion of 1.05E-5 1/K at 200.0 °C | 200.0 °C | for 20°C to the mentioned temperature | |
1.08E-5 1/K Show Supplier Material materials with Coefficient of thermal expansion of 1.08E-5 1/K at 300.0 °C | 300.0 °C | for 20°C to the mentioned temperature | |
1.12E-5 1/K Show Supplier Material materials with Coefficient of thermal expansion of 1.12E-5 1/K at 400.0 °C | 400.0 °C | for 20°C to the mentioned temperature | |
1.13E-5 1/K Show Supplier Material materials with Coefficient of thermal expansion of 1.13E-5 1/K at 500.0 °C | 500.0 °C | for 20°C to the mentioned temperature | |
1.14E-5 1/K Show Supplier Material materials with Coefficient of thermal expansion of 1.14E-5 1/K at 600.0 °C | 600.0 °C | for 20°C to the mentioned temperature | |
1.16E-5 1/K Show Supplier Material materials with Coefficient of thermal expansion of 1.16E-5 1/K at 700.0 °C | 700.0 °C | for 20°C to the mentioned temperature | |
Specific heat capacity | 420 J/(kg·K) Show Supplier Material materials with Specific heat capacity of 420 J/(kg·K) at 23.0 °C | 23.0 °C | |
Thermal conductivity | 22.2 W/(m·K) Show Supplier Material materials with Thermal conductivity of 22.2 W/(m·K) at 20.0 °C | 20.0 °C |
Electrical
Property | Value | Temperature |
---|---|---|
Electrical resistivity | 6.1E-7 Ω·m Show Supplier Material materials with Electrical resistivity of 6.1E-7 Ω·m at 23.0 °C | 23.0 °C |
Chemical properties
Property | ||
---|---|---|
Carbon | 1.3 % | |
Chromium | 4.2 % | |
Cobalt | 8.5 % | |
Iron | Balance | |
Molybdenum | 5 % | |
Tungsten | 6.4 % | |
Vanadium | 3 % |
Technological properties
Property | ||
---|---|---|
Application areas | Thread-cutting tools, reamers, heavy-duty milling cutters, drills, punching tools |