DIN EN ISO HS6-7-6-10, 1.3241 / 1.3292
Want to keep this datasheet? Save it now in your required format

Description

1.3241/1.3292 (HS6-7-6-10) high speed tool steel, W and Co alloyed, with increased volume fraction of carbides for highest wear resistance also at elevated temperatures.

Equivalent Materials

This material data has been provided by Deutsche Edelstahlwerke Specialty Steel (DEW).

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyValue

Density

7.9 g/cm³

Show Supplier Material materials with Density of 7.9 g/cm³

Mechanical

PropertyValue

Elastic modulus

250 GPa

Show Supplier Material materials with Elastic modulus of 250 GPa

Hardness, Rockwell C

63.0 - 69.0 [-]

Show Supplier Material materials with Hardness, Rockwell C of 63.0 - 69.0 [-]

Thermal

PropertyTemperatureValueComment

Coefficient of thermal expansion

100 °C

0.0000101 1/K

Show Supplier Material materials with Coefficient of thermal expansion of 0.0000101 1/K

for 20°C to the mentioned temperature

200 °C

0.0000103 1/K

Show Supplier Material materials with Coefficient of thermal expansion of 0.0000103 1/K

for 20°C to the mentioned temperature

300 °C

0.0000106 1/K

Show Supplier Material materials with Coefficient of thermal expansion of 0.0000106 1/K

for 20°C to the mentioned temperature

400 °C

0.0000108 1/K

Show Supplier Material materials with Coefficient of thermal expansion of 0.0000108 1/K

for 20°C to the mentioned temperature

600 °C

0.0000111 1/K

Show Supplier Material materials with Coefficient of thermal expansion of 0.0000111 1/K

for 20°C to the mentioned temperature

Specific heat capacity

420.0 J/(kg·K)

Show Supplier Material materials with Specific heat capacity of 420.0 J/(kg·K)

Thermal conductivity

20 °C

22.5 W/(m·K)

Show Supplier Material materials with Thermal conductivity of 22.5 W/(m·K)

Chemical properties

PropertyValue

Carbon

2.3

Show Supplier Material materials with Carbon of 2.3

Chromium

4.2

Show Supplier Material materials with Chromium of 4.2

Cobalt

10.5

Show Supplier Material materials with Cobalt of 10.5

Molybdenum

7.0

Show Supplier Material materials with Molybdenum of 7.0

Tungsten

7.0

Show Supplier Material materials with Tungsten of 7.0

Vanadium

6.5

Show Supplier Material materials with Vanadium of 6.5

Technological properties

Property
Application areas

Heavy-duty cutting tools with very high requirements on red hardness and wear resistance