APTIV® 1000 series films are the unfilled semi-crystalline films made from VICTREX® PEEK polymer. The film provides a material solution for engineers in ultra-high performance applications.


APTIV films are a comprehensive range of versatile, high-performance films, the use of which can facilitate reduced systems costs, improved performance and enhanced design freedom.


APTIV 1000 has a unique combination of properties providing high temperature performance, lightweight, mechanical strength, durability, excellent radiation, hydrolysis and chemical resistance, electrical insulation, wear and abrasion resistance, excellent barrier properties with high purity, good flammability without the use of flame retardants, low toxicity of combustion products, and low moisture absorption in a film format. Inherently halogen-free and ease of processing makes APTIV films a technology enabler for our customers and end users.

Properties

Dimension

Thickness t

0.13 mm

Mechanical

Elastic modulus E

2.3 GPa at 23 °C

ISO 527

Elastic modulus, transverse E

2.3 GPa at 23 °C

ISO 527

Elongation A

150 % at 23 °C

ISO 527

Elongation, transverse A

150 % at 23 °C

ISO 527

Tensile strength Rm

120 MPa at 23 °C

ISO 527

Tensile strength, transverse Rm,trans

120 MPa at 23 °C

ISO 527

Electrical

Breakdown voltage Ubreak

15 kV at 23 °C

ASTM D149 (6.25mm electrode)

Dielectric strength EDS

120 kV/mm at 20 °C

ASTM D149 (6.25mm electrode)

Technological properties

Application areas

Electrical insulation, pressure sensitive tapes, printed circuit substrates, high temperature labels, washers in high speed motors, washers in mobile phone hinges, flexible surface heaters, aerospace insulation, pressure sensor membranes, acoustic speaker diaphragms, capacitors, composites, proven temperature resistance to use of lead free solders

Compliance

APTIV® film is FDA and EU approved for food contact and is RoHS and 3A Sanitary Standards compliant.

Other

The key features are: High heat resistance, excellent tribological properties, broad chemical resistance, low moisture absorption, high strength and toughness, stable and excellent electrical insulation properties, good flammability performance without use of flame retardant additives, inherently halogen-free, radiation resistance, low smoke and toxic gas emission, excellent hydrolysis resistance, excellent barrier properties, excellent acoustic properties, high purity, lightweight, recyclable, easy to process

Processing methods

Can be laminated to other materials thermoformed, metallised, coated, printed, stamped and die cut, welded and heat sealed and coated.

This material data has been provided by Goodfellow.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.