Dimension
Property | Value |
---|---|
Thickness | 0.03 mm Show Material materials with Thickness of 0.03 mm |
Mechanical
Property | Temperature | Value | Comment |
---|---|---|---|
Elastic modulus | 23.0 °C | 1.8 GPa Show Material materials with Elastic modulus of 1.8 GPa | ISO 527 |
Elastic modulus, transverse | 23.0 °C | 1.8 GPa Show Material materials with Elastic modulus, transverse of 1.8 GPa | ISO 527 |
Elongation | 23.0 °C | 200 % Show Material materials with Elongation of 200 % | ISO 527 |
Elongation, transverse | 23.0 °C | 200 % Show Material materials with Elongation, transverse of 200 % | ISO 527 |
Tensile strength | 23.0 °C | 130 MPa Show Material materials with Tensile strength of 130 MPa | ISO 527 |
Tensile strength, transverse | 23.0 °C | 130 MPa Show Material materials with Tensile strength, transverse of 130 MPa | ISO 527 |
Thermal
Property | Value |
---|---|
Glass transition temperature | 143 °C Show Material materials with Glass transition temperature of 143 °C |
Electrical
Technological properties
Property | ||
---|---|---|
Application areas | Aerospace insulation, electrical insulation, acoustic speaker diaphragms, thermoforming of thin wall parts, composites | |
Certifications | APTIV 2000 film is approved for Food Contact Use: APTIV 2000 film is compliant with the compositional requirements of FDA 21 CFR 177.2415. APTIV 2000 film is compliant with the framework regulation (EC) No. 1935/2004/EC and commission directive 2002/72/EC and the amendments up to 2005/79/EC. APTIV 2000 film is fully compliant with the 3-A Sanitary Standards. APTIV film 2000 complies with the requirements of RoHS European Directive 2002/95/EC and can be used to manufacture products compliant with the same directive. APTIV 2000 film is inherently halogen-free in accordance with IEC61249-2-21. | |
Other | The key features are: High heat resistance, excellent Flexural fatigue properties, broad chemical resistance, low moisture absorption, high strength and toughness, stable and excellent electrical insulation properties, good flammability performance without use of flame retardant additives, inherently halogen-free, radiation resistance, low smoke and toxic gas emission, excellent hydrolysis resistance, excellent acoustic properties, high purity, lightweight, recyclable, easy to process. | |
Processing methods | Can be laminated to other materials thermoformed, metallised, coated, printed, stamped and die cut, welded and heat sealed and coated. APTIV 2000 film can easily be subjected to a range of secondary process operations, which allow designers and engineers to obtain the benefits of APTIV film properties in a variety of forms: Surface treatment, adhesion, coatings, slitting, die cutting and stamping, thermal lamination, heat welding and heat sealing, metallisation, laser marking and machining, thermoforming, printing |