Härte, Brinell: 143 - 187 [-]

Quick Comparison

7000 Serie

WL 3.4364-1 Grade 3.4365 T6

Geliefert von:

3 Matmatch-Lieferanten

7000 Serie

WL 3.4364-1 Grade 3.4365 T6

Geliefert von:

3 Matmatch-Lieferanten

7000 Serie

AA Standards Grade 7075 T6

Geliefert von:

3 Matmatch-Lieferanten

7000 Serie

AA Standards Grade 7075 T651

Geliefert von:

3 Matmatch-Lieferanten

Nickel Chromium Iron Alloy

VDM® Alloy 600 H

Geliefert von:

VDM Metals

Cast Copper Brass Yellow Brass

ASTM B505 Grade C86200

Geliefert von:

1 Matmatch-Lieferant

Cast Copper Bronze Aluminium Bronze

ASTM B505 Grade C95300 Heat-Treated

Geliefert von:

1 Matmatch-Lieferant

Cast Copper Bronze Aluminium Bronze

ASTM B505 Grade C95300 HT, Heat-Treated

Geliefert von:

1 Matmatch-Lieferant

Cast Copper Bronze Aluminium Bronze

ASTM B505 Grade C95500 Heat-Treated

Geliefert von:

1 Matmatch-Lieferant

Cast Copper Bronze Aluminium Bronze

ASTM B505 Grade C95500 HT, Heat-Treated

Geliefert von:

1 Matmatch-Lieferant

Cast Copper Bronze Aluminium Bronze

ASTM B505 Grade C95520

Geliefert von:

1 Matmatch-Lieferant

Cast Copper Brass Yellow Brass

ASTM B584 Grade C86700

Geliefert von:

1 Matmatch-Lieferant

Seite 1 von 48