Acero inoxidable austenítico
Esshete 1250Suministrada por:
Alleima (formerly Sandvik Materials Technology)Acero inoxidable austenítico
Sanicro® 25Suministrada por:
Alleima (formerly Sandvik Materials Technology)Superaustenitic Stainless Steel
Sandvik 353 MASuministrada por:
Alleima (formerly Sandvik Materials Technology)Acero inoxidable ferrítico
DIN 17440 Grade X6Cr17 soft annealed (+A)Acero inoxidable austenítico
EN 10088-1 Grade X2CrNiMoN17-13-5 solution annealed (+AT)Acero inoxidable austenítico
EN 10088-1 Grade X1CrNiMoN25-22-2 solution annealed (+AT)Acero inoxidable austenítico
EN 10088-1 Grade X2CrNiMoN17-13-3 solution annealed (+AT)Acero inoxidable austenítico
EN 10088-1 Grade X2CrNiN18-10 solution annealed (+AT)