Acero inoxidable martensítico
ASTM A841 Grade A Class 1 Thermo-Mechanical Control Process (TMCP)Suministrada por:
1 proveedor Matmatch
Cast Copper Bronze Aluminium Bronze
ASTM B505 Grade C95300 Heat-TreatedSuministrada por:
1 proveedor Matmatch
Cast Copper Bronze Aluminium Bronze
ASTM B505 Grade C95300 HT, Heat-TreatedSuministrada por:
1 proveedor Matmatch
Cast Copper Bronze Aluminium Bronze
ASTM B505 Grade C95500 Heat-TreatedSuministrada por:
1 proveedor Matmatch
Cast Copper Bronze Aluminium Bronze
ASTM B505 Grade C95500 HT, Heat-TreatedSuministrada por:
1 proveedor Matmatch
Acero inoxidable ferrítico
DIN 17440 Grade X6Cr17 soft annealed (+A)Acero inoxidable ferrítico
DIN 17440 Grade X3CrTi17 soft annealed (+A)Acero inoxidable ferrítico
DIN 17440 Grade X6CrAl13 soft annealed (+A)Acero inoxidable austenítico
DIN 17440 Grade X5CrNi18-10 quenched (+Q)Acero inoxidable ferrítico
EN 10088-1 Grade X3CrNb17 soft annealed (+A)Acero inoxidable austenítico
DIN 17440 Grade X5CrNi18-10 solution heat-treated and quenchedAcero inoxidable austenítico
EN 10028-7 Grade X5CrNi18-10 solution annealed (+AT)Acero inoxidable austenítico
EN 10272 Grade X5CrNi18-10 solution annealed (+AT)