Conductividad térmica: 18.8 W/(m·K)

Quick Comparison

Nickel Chromium Iron Alloy

VDM® Alloy 718

Suministrada por:

VDM Metals

Acero inoxidable martensítico

ASTM A841 Grade A Class 1 Thermo-Mechanical Control Process (TMCP)

Suministrada por:

1 proveedor Matmatch

Nickel Steel

ASTM A353 Double-Normalized and Tempered

Suministrada por:

1 proveedor Matmatch

Tin Bronze

ASTM B505 Grade C90700

Suministrada por:

1 proveedor Matmatch

Leaded Tin Bronze

ASTM B505 Grade C92700

Suministrada por:

1 proveedor Matmatch

Cast Copper Bronze Aluminium Bronze

ASTM B505 Grade C95200

Suministrada por:

1 proveedor Matmatch

Cast Copper Bronze Aluminium Bronze

ASTM B505 Grade C95300 Heat-Treated

Suministrada por:

1 proveedor Matmatch

Cast Copper Bronze Aluminium Bronze

ASTM B505 Grade C95300 HT, Heat-Treated

Suministrada por:

1 proveedor Matmatch

Cast Copper Bronze Aluminium Bronze

ASTM B505 Grade C95500 Heat-Treated

Suministrada por:

1 proveedor Matmatch

Cast Copper Bronze Aluminium Bronze

ASTM B505 Grade C95500 HT, Heat-Treated

Suministrada por:

1 proveedor Matmatch

Cast Copper Bronze Aluminium Bronze

ASTM B505 Grade C95520

Suministrada por:

1 proveedor Matmatch

Compuesto de matriz férrea

Ferro-Titanit® S

Suministrada por:

Deutsche Edelstahlwerke (DEW)

Compuesto de matriz férrea

Ferro-Titanit® Nikro 128

Suministrada por:

Deutsche Edelstahlwerke (DEW)

Compuesto de matriz férrea

Ferro-Titanit® Nikro 143

Suministrada por:

Deutsche Edelstahlwerke (DEW)
Página 1 de 162