Description

The UHMWPE fiber from DSM Dyneema is a gel-spun, multi-filament fiber produced from ultra high molecular weight polyethylene, with main characteristics:


  • High strength
  • Low weight
  • Low elongation at break
  • Resistance to most chemicals
  • This material data has been provided by Matmatch.

    All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
    Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

    Ashby charts

    See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

    Properties

    General

    PropertyTemperatureValueComment

    Density

    20.0 °C

    0.97 - 0.98 g/cm³

    Show Material materials with Density of 0.97 - 0.98 g/cm³

    Limiting oxygen index

    20.0 °C

    20 %

    Show Material materials with Limiting oxygen index of 20 %

    min.

    Mechanical

    PropertyTemperatureValue

    Compressive strength

    20.0 °C

    0.1 MPa

    Show Material materials with Compressive strength of 0.1 MPa

    Compressive strength, transverse

    20.0 °C

    0.1 MPa

    Show Material materials with Compressive strength, transverse of 0.1 MPa

    Elastic modulus

    20.0 °C

    94 GPa

    Show Material materials with Elastic modulus of 94 GPa

    Elastic modulus, transverse

    20.0 °C

    3 GPa

    Show Material materials with Elastic modulus, transverse of 3 GPa

    Elongation

    20.0 °C

    3 - 4 %

    Show Material materials with Elongation of 3 - 4 %

    Tensile strength

    20.0 °C

    3100 MPa

    Show Material materials with Tensile strength of 3100 MPa

    Tensile strength, transverse

    20.0 °C

    30 MPa

    Show Material materials with Tensile strength, transverse of 30 MPa

    Thermal

    PropertyTemperatureValue

    Coefficient of thermal expansion

    20.0 °C

    -1.2E-5 1/K

    Show Material materials with Coefficient of thermal expansion of -1.2E-5 1/K

    Melting point

    300 °C

    Show Material materials with Melting point of 300 °C

    Specific heat capacity

    20.0 °C

    1850 J/(kg·K)

    Show Material materials with Specific heat capacity of 1850 J/(kg·K)

    Thermal conductivity

    20.0 °C

    20 W/(m·K)

    Show Material materials with Thermal conductivity of 20 W/(m·K)

    Thermal conductivity, transverse

    20.0 °C

    0.2 W/(m·K)

    Show Material materials with Thermal conductivity, transverse of 0.2 W/(m·K)

    Electrical

    PropertyTemperatureValue

    Dielectric constant, 10GHz

    20.0 °C

    2.25 [-]

    Show Material materials with Dielectric constant, 10GHz of 2.25 [-]

    Dielectric strength

    20.0 °C

    900 kV/mm

    Show Material materials with Dielectric strength of 900 kV/mm

    Electrical resistivity

    20.0 °C

    1.00E+14 Ω·m

    Show Material materials with Electrical resistivity of 1.00E+14 Ω·m

    Loss factor

    20.0 °C

    2E-4 [-]

    Show Material materials with Loss factor of 2E-4 [-]

    Optical

    PropertyTemperatureValue

    Birefringence

    20.0 °C

    0.06 nm/cm

    Show Material materials with Birefringence of 0.06 nm/cm

    Refractive index

    1.59 [-]

    Show Material materials with Refractive index of 1.59 [-]

    Technological properties

    Property
    Application areas

    Deep water mooring lines, Standing rigging ropes