Description

  • high dimensional accuracy and stability
  • very high strength
  • good chemical resistance
  • very high rigidity
  • easy to weld and stick
  • not hot water resistant above 60 ° C
  • This material data has been provided by Matmatch.

    All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
    Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

    Ashby charts

    See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

    Properties

    General

    PropertyTemperatureValue

    Density

    23.0 °C

    1.46 g/cm³

    Show Material materials with Density of 1.46 g/cm³

    Mechanical

    PropertyTemperatureValueComment

    Elastic modulus

    23.0 °C

    3.4 GPa

    Show Material materials with Elastic modulus of 3.4 GPa

    DIN EN ISO 527-2

    Elongation

    23.0 °C

    6 %

    Show Material materials with Elongation of 6 %

    DIN EN ISO 527-2

    Flexural modulus

    23.0 °C

    3.4 GPa

    Show Material materials with Flexural modulus of 3.4 GPa

    DIN EN ISO 178

    Flexural strength

    23.0 °C

    78 MPa

    Show Material materials with Flexural strength of 78 MPa

    DIN EN ISO 178

    Tensile strength

    23.0 °C

    46 MPa

    Show Material materials with Tensile strength of 46 MPa

    DIN EN ISO 527-2

    Yield strength

    23.0 °C

    46 MPa

    Show Material materials with Yield strength of 46 MPa

    DIN EN ISO 527-2

    Thermal

    PropertyTemperatureValueComment

    Coefficient of thermal expansion

    60.0 °C

    8E-5 1/K

    Show Material materials with Coefficient of thermal expansion of 8E-5 1/K

    ISO 11359-1/2, value between 23°C and the mentioned Temperature

    100.0 °C

    1E-4 1/K

    Show Material materials with Coefficient of thermal expansion of 1E-4 1/K

    ISO 11359-1/2, value between 23°C and the mentioned Temperature

    Max service temperature

    200 °C

    Show Material materials with Max service temperature of 200 °C

    Shortterm

    Melting point

    224 °C

    Show Material materials with Melting point of 224 °C

    DIN EN ISO 11357

    Min service temperature

    110 °C

    Show Material materials with Min service temperature of 110 °C

    Longterm

    Specific heat capacity

    23.0 °C

    1.2E-3 J/(kg·K)

    Show Material materials with Specific heat capacity of 1.2E-3 J/(kg·K)

    ISO 22007-4

    Thermal conductivity

    23.0 °C

    0.33 W/(m·K)

    Show Material materials with Thermal conductivity of 0.33 W/(m·K)

    ISO 22007-4

    Flammability

    HB UL94

    Electrical

    PropertyTemperatureValueComment

    Surface resistivity

    23.0 °C

    1.00E+14 Ω/sq

    Show Material materials with Surface resistivity of 1.00E+14 Ω/sq

    DIN IEC 60093

    Technological properties

    Property
    Application areas

    General Automotive Parts, Electronic devices

    Fillers

    30% Glass Fiber

    Processing methods

    Injection Molded