Cycolac™ MG47F resin

Want to keep this datasheet? Save it now in your required format

Description

Cycolac™ is a range of thermoplastic resin products, developed by Sabic, which is made of acrylonitrile-butadiene-styrene (ABS). It has excellent colourability and can be found in a wide range of colours, offering outstanding aesthetics. They have highly tailorable engineering properties and outstanding flow, toughness, dimensional stability, scratch resistance, and high-temperature resistance.
Cycolac™ MG47F resin is a multi-purpose ABS for injection moulding. It is FDA approved. As a multi-purpose material, it provides a favourable balance of engineering properties. Its key features include:

  • Excellent aesthetics
  • High toughness
  • Good dimensional stability
  • High scratch resistance
  • High temperature resistance
  • Excellent colourability
  • Good fatigue and chemical resistance

This material data has been provided by Matmatch.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

See where falls on the material property chart for against in your materials selection and design process. Our Ashby charts are interactive with more technical data upon clicking. Sign up to get access to this premium feature for free.

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

1.04 g/cm³

Show Material materials with Density of 1.04 g/cm³

ASTM D792

Mechanical

PropertyTemperatureValueComment

Elastic modulus

23.0 °C

2.27 GPa

Show Material materials with Elastic modulus of 2.27 GPa

ASTM D790

Elongation

23.0 °C

24 %

Show Material materials with Elongation of 24 %

ASTM D638

Elongation at yield

23.0 °C

2 %

Show Material materials with Elongation at yield of 2 %

ASTM D638

Flexural modulus

23.0 °C

2.3 GPa

Show Material materials with Flexural modulus of 2.3 GPa

ASTM D790

Flexural yield strength

23.0 °C

70 MPa

Show Material materials with Flexural yield strength of 70 MPa

ASTM D790

Impact strength, Charpy notched

-30.0 °C

9 kJ/m²

Show Material materials with Impact strength, Charpy notched of 9 kJ/m²

ISO 179/1eA

23.0 °C

26 kJ/m²

Show Material materials with Impact strength, Charpy notched of 26 kJ/m²

ISO 179/1eA

Impact strength, Izod notched

-30.0 °C

8 kJ/m²

Show Material materials with Impact strength, Izod notched of 8 kJ/m²

ISO 180/1A

23.0 °C

22 kJ/m²

Show Material materials with Impact strength, Izod notched of 22 kJ/m²

ISO 180/1A

Unlock all property charts

Impact strength, Izod notched, ASTM

23.0 °C

320 J/m

Show Material materials with Impact strength, Izod notched, ASTM of 320 J/m

ASTM D256

Tensile strength

23.0 °C

33 MPa

Show Material materials with Tensile strength of 33 MPa

ASTM D638

Yield strength

23.0 °C

44 MPa

Show Material materials with Yield strength of 44 MPa

ASTM D638

Thermal

PropertyTemperatureValueComment

Coefficient of thermal expansion

23.0 °C

8.82E-5 1/K

Show Material materials with Coefficient of thermal expansion of 8.82E-5 1/K

ASTM E831, for -40 to 40°C

Coefficient of thermal expansion, transverse

23.0 °C

8.82E-5 1/K

Show Material materials with Coefficient of thermal expansion, transverse of 8.82E-5 1/K

ASTM E831, for -40 to 40°C

Heat deflection temperature, 0.45 MPa

94 °C

Show Material materials with Heat deflection temperature, 0.45 MPa of 94 °C

ASTM D648

Heat deflection temperature, 1.80 MPa

80 °C

Show Material materials with Heat deflection temperature, 1.80 MPa of 80 °C

ASTM D648

Melting point

220 - 260 °C

Show Material materials with Melting point of 220 - 260 °C

Relative temperature index, electrical

60 °C

Show Material materials with Relative temperature index, electrical of 60 °C

UL 746

Relative temperature index, mechanical strength

60 °C

Show Material materials with Relative temperature index, mechanical strength of 60 °C

UL 746

Vicat softening temperature

98 °C

Show Material materials with Vicat softening temperature of 98 °C

ISO 906, Rate B/50

Flammability

UL Recognized, 94HB Flame Class Rating (3) 1.5 mm UL 94

Rheological Properties

PropertyValueComment

Melt mass-flow rate

5.6 g/10min

Show Material materials with Melt mass-flow rate of 5.6 g/10min

ASTM D1238 230°C/3.8 kgf

Melt volume-flow rate

18 cm³/10min

Show Material materials with Melt volume-flow rate of 18 cm³/10min

ISO 1133, 220°C/10.0 kg

Technological properties

Property
Application areas

Additive manufacturing, Appliances, Automotive exterior parts, Construction applications, Electronic displays, Fluid handling, Lawn and garden equipment, Lenses, Lighting applications, medical/healthcare, Non-specific food, Outdoor applications, packaging

Color

Black, White, Natural (unpigmented)

Processing methods

Injection Molding: Drying Temperature: 80-95°C, Drying Time: 2-4 hr, Rear Temperature: 190-210°C, Middle Temperature: 205-225°C, Front Temperature: 215-240°C, Nozzle Temperature: 220-260°C, Melt Temperature: 220-260°C, Mold Temperature: 50-70°C, Back Pressure: 0.3-0.7 MPa, Screw Speed 30-60 rpm