3M™ Dyneon™ (Fluoroplastic PVDF 315080003)

Want to keep this datasheet? Save it now in your required format

Description

PVDF 315080003 is a flexible copolymer of vinylidene fluoride (VF2) and chlorotrifluoroethylene (CTFE), exhibiting very low shrinkage and excellent impact resistance. PVDF 315080003 also has a very low brittleness temperature, for excellent low temperature performance. As with all PVDF grades, PVDF 315080003 also possesses very good chemical and temperature resistance.


Special Features are:

  • Copolymer of vinylidene fluoride (VF2) and chlorotrifluoroethylene (CTFE)
  • Ultra-flexible
  • Very low shrinkage rates
  • Wide operating temperature range
  • Processable using a variety of thermoplastic conversion techniques
  • Excellent low flame and low smoke performance

  • Typical Properties:

    PVDF 315080003 has excellent flame and smoke performance, with an LOI of 65.

    This material data has been provided by Matmatch.

    All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
    Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

    Ashby charts

    Properties

    General

    PropertyValueComment

    Density

    1.76 g/cm³

    Show Material materials with Density of 1.76 g/cm³

    ISO 1183

    Limiting oxygen index

    65 %

    Show Material materials with Limiting oxygen index of 65 %

    ASTM D2863

    Water absorption

    0.04 %

    Show Material materials with Water absorption of 0.04 %

    ISO 62 (Method 1, 24hr @ 23°C), maximum

    Equilibrium

    Saturation

    Mechanical

    PropertyValueComment

    Elongation

    475 %

    Show Material materials with Elongation of 475 %

    ASTM D638, 23 °C, 50 mm/min

    Flexural modulus

    0.425 GPa

    Show Material materials with Flexural modulus of 0.425 GPa

    ASTM D790

    Tensile strength

    22 MPa

    Show Material materials with Tensile strength of 22 MPa

    ASTM D638, 23 °C, 50 mm/min

    Thermal

    PropertyValueComment

    Brittleness temperature

    -37 °C

    Show Material materials with Brittleness temperature of -37 °C

    ASTM D257

    Melting point

    169 °C

    Show Material materials with Melting point of 169 °C

    ASTM D3418

    Flammability

    V-0 UL94

    Electrical

    PropertyValueComment

    Dielectric constant

    7 [-]

    Show Material materials with Dielectric constant of 7 [-]

    ASTM D150, 1 MHz

    Electrical resistivity

    1e+12 Ω·m

    Show Material materials with Electrical resistivity of 1e+12 Ω·m

    DIN 53483, minimum

    Surface resistivity

    1e+14 Ω/sq

    Show Material materials with Surface resistivity of 1e+14 Ω/sq

    DIN 53483, 23 °C, minimum

    Rheological Properties

    PropertyValueComment

    Melt mass-flow rate

    15.5 g/10min

    Show Material materials with Melt mass-flow rate of 15.5 g/10min

    ASTM D1238, 230 °C, 5kg, 2.16 kg

    Technological properties

    Property
    Application areas

    PVDF 315080003 is ideal for insulation and buffering materials for wire and cable applications and for tubing.

    Processing methods

    Injection Molding