PS 100 is general purpose Polystyrene manufactured by continuous mass polymerization of styrene monomer. It is a crystal-like, hard and brittle polymer with good flow properties and high clarity. It is designed for medium and thin wall thickness articles and gives broad processing window for molding applications.

This material data has been provided by Matmatch.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValueComment

Bulk density

23.0 °C

0.6 g/cm³

Show Material materials with Bulk density of 0.6 g/cm³

ASTM D 1895

Mechanical

PropertyTemperatureValueComment

Elastic modulus

23.0 °C

2.25 GPa

Show Material materials with Elastic modulus of 2.25 GPa

ASTM D638

Elongation

23.0 °C

2 %

Show Material materials with Elongation of 2 %

ASTM D638

Flexural modulus

23.0 °C

3.53 GPa

Show Material materials with Flexural modulus of 3.53 GPa

ASTM D 790

Flexural strength

23.0 °C

72 MPa

Show Material materials with Flexural strength of 72 MPa

ASTM D790

Hardness, Rockwell L

23.0 °C

94 [-]

Show Material materials with Hardness, Rockwell L of 94 [-]

ASTM D785

Impact strength, Izod notched, ASTM

23.0 °C

12 J/m

Show Material materials with Impact strength, Izod notched, ASTM of 12 J/m

ASTM D256A

Tensile strength

23.0 °C

40 MPa

Show Material materials with Tensile strength of 40 MPa

ASTM D638

Thermal

PropertyValueComment

Heat deflection temperature, 0.45 MPa

90 °C

Show Material materials with Heat deflection temperature, 0.45 MPa of 90 °C

ASTM D648

Vicat softening temperature

95 °C

Show Material materials with Vicat softening temperature of 95 °C

ASTM D 1525 | Rate A/50°C

Rheological Properties

PropertyValueComment

Melt mass-flow rate

14 g/10min

Show Material materials with Melt mass-flow rate of 14 g/10min

ASTM D 1238 | 230°C/2.16 kg

Technological properties

Property
Application areas

Multi purpose injection moulding