SABIC® PS 160

Want to keep this datasheet? Save it now in your required format

Description

General purpose Polystyrene PS 160 is manufactured by continuous mass polymerization of styrene monomer. It is a crystal-like, hard and brittle material having High molecular weight imparting high tensile strength to end- products. It has high vicat and heat deflection temperatures.

This material data has been provided by Matmatch.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValueComment

Bulk density

23.0 °C

0.6 g/cm³

Show Material materials with Bulk density of 0.6 g/cm³

ASTM D 1895

Mechanical

PropertyTemperatureValueComment

Elastic modulus

23.0 °C

2.99 GPa

Show Material materials with Elastic modulus of 2.99 GPa

ASTM D638

Elongation

23.0 °C

2 %

Show Material materials with Elongation of 2 %

ASTM D638

Flexural modulus

23.0 °C

3.63 GPa

Show Material materials with Flexural modulus of 3.63 GPa

ASTM D 790

Flexural strength

23.0 °C

95 MPa

Show Material materials with Flexural strength of 95 MPa

ASTM D790

Impact strength, Izod notched, ASTM

23.0 °C

20 J/m

Show Material materials with Impact strength, Izod notched, ASTM of 20 J/m

ASTM D256A

Tensile strength

23.0 °C

51 MPa

Show Material materials with Tensile strength of 51 MPa

ASTM D638

Thermal

PropertyValueComment

Heat deflection temperature, 0.45 MPa

100 °C

Show Material materials with Heat deflection temperature, 0.45 MPa of 100 °C

ASTM D648

Vicat softening temperature

104 °C

Show Material materials with Vicat softening temperature of 104 °C

ASTM D 1525 | Rate A/50°C

Rheological Properties

PropertyValueComment

Melt mass-flow rate

3.3 g/10min

Show Material materials with Melt mass-flow rate of 3.3 g/10min

ASTM D 1238 | 200°C/5 kg

Technological properties

Property
Application areas

Food Container