XENOY™ Resin 5720

Want to keep this datasheet? Save it now in your required format

Description

UR, PBT+PC alloy. Outstanding low temperature impact/chemical resistance.

This material data has been provided by Matmatch.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

1.17 g/cm³

Show Material materials with Density of 1.17 g/cm³

ASTM D 792

Water absorption

23.0 °C

0.13 %

Show Material materials with Water absorption of 0.13 %

ASTM D 570 | 24 Hours

Mechanical

PropertyTemperatureValueComment

Elongation

23.0 °C

165 %

Show Material materials with Elongation of 165 %

ASTM D 638 | Type I, 50 mm/min

Flexural modulus

23.0 °C

1.72 GPa

Show Material materials with Flexural modulus of 1.72 GPa

ASTM D 790 | 1.3 mm/min, 50 mm span

Flexural yield strength

23.0 °C

68 MPa

Show Material materials with Flexural yield strength of 68 MPa

ASTM D 790 | 1.3 mm/min, 50 mm span

Impact strength, Izod notched, ASTM

-40.0 °C

534 J/m

Show Material materials with Impact strength, Izod notched, ASTM of 534 J/m

ASTM D 256

23.0 °C

801 J/m

Show Material materials with Impact strength, Izod notched, ASTM of 801 J/m

ASTM D 256

Impact strength, Izod unnotched, ASTM

23.0 °C

3204 J/m

Show Material materials with Impact strength, Izod unnotched, ASTM of 3204 J/m

ASTM D 4812

Yield strength

23.0 °C

49 MPa

Show Material materials with Yield strength of 49 MPa

ASTM D 638 | Type I, 50 mm/min

Thermal

PropertyValueComment

Heat deflection temperature, 1.80 MPa

96 °C

Show Material materials with Heat deflection temperature, 1.80 MPa of 96 °C

ASTM D 648 | 1.82 MPa, 6.4 mm, unannealed

Relative temperature index, electrical

75 °C

Show Material materials with Relative temperature index, electrical of 75 °C

UL 746B

Relative temperature index, mechanical impact

75 °C

Show Material materials with Relative temperature index, mechanical impact of 75 °C

UL 746B

Relative temperature index, mechanical strength

75 °C

Show Material materials with Relative temperature index, mechanical strength of 75 °C

UL 746B

Flammability

UL Recognized, 94HB Flame Class Rating | 1.49mm | UL 94

Electrical

PropertyTemperatureValueComment

Dielectric constant

23.0 °C

2.95 [-]

Show Material materials with Dielectric constant of 2.95 [-]

ASTM D 150 | at 1 MHz

Dielectric strength

23.0 °C

19.8 kV/mm

Show Material materials with Dielectric strength of 19.8 kV/mm

ASTM D 149 | in air, 3.2 mm

Dissipation factor

23.0 °C

0.03 [-]

Show Material materials with Dissipation factor of 0.03 [-]

ASTM D 150 | at 1 MHz

Electrical resistivity

23.0 °C

9.50E+14 Ω·m

Show Material materials with Electrical resistivity of 9.50E+14 Ω·m

ASTM D 257

Rheological Properties

PropertyTemperatureValueComment

Shrinkage

23.0 °C

1 - 1.2 %

Show Material materials with Shrinkage of 1 - 1.2 %

SABIC method | 3.2 mm

Technological properties

Property
Application areas

Amusement Machine,ATM/Ticket Machine,Audio,Data Transfer,Document Handling,Electronic Components,Enclosure/Housing/Cover,Industrial Material Handling,Lab Ware and Clinical Diagnostics,Medical Device,Personal Computing,Photovoltaic Components,Security/Detection

Processing methods

Drying Temperature: 110°C, Drying Time: 4-6hrs, Drying Time (Cumulative): 8hrs, Maximum Moisture Content: 0.02%, Melt Temperature: 260-275°C, Nozzle Temperature: 255-270°C, Front - Zone 3 Temperature: 255-275°C, Middle - Zone 2 Temperature: 250-270°C, Rear - Zone 1 Temperature: 245-265°C, Mold Temperature: 65-90°C, Back Pressure: 0.3-0.7MPa, Screw Speed: 50-80rpm, Shot to Cylinder Size: 50-80%, Vent Depth: 0.013-0.02mm