SABIC® SUPEER™ 8112

Want to keep this datasheet? Save it now in your required format

Description

SABIC® SUPEER™ 8112 is an ethylene-octene copolymer produced via solution polymerization using metallocene catalyst. It performs well in a wide range of general purpose and high performance LLDPE blown film applications and have excellent processability.

This material data has been provided by Matmatch.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

0.91 g/cm³

Show Material materials with Density of 0.91 g/cm³

ASTM D1505

Thermal

PropertyValueComment

Melting point

111 °C

Show Material materials with Melting point of 111 °C

SABIC method

Optical

PropertyValueComment

Haze

7 %

Show Material materials with Haze of 7 %

ASTM D1003

Technological properties

Property
Application areas

Stretch film,Lamination film,Heavy duty film