SABIC® COHERE™ 8185 is an ethylene-octene copolymer produced via solution polymerization using metallocene catalyst. It performs well in high performance film applications with outstanding gel control, and an excellent combination of toughness, hot tack, sealing and optical properties.

This material data has been provided by Matmatch.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

Mechanical

PropertyTemperatureValueComment

Flexural modulus

23.0 °C

29.4 GPa

Show Material materials with Flexural modulus of 29.4 GPa

ASTM D790 A

Tear strength

23.0 °C

58.5 kN/m

Show Material materials with Tear strength of 58.5 kN/m

ASTM D624

Thermal

PropertyValueComment

Melting point

74 °C

Show Material materials with Melting point of 74 °C

SABIC method

Technological properties

Property
Application areas

Blown film