SABIC® SUPEER™ 8315

Want to keep this datasheet? Save it now in your required format

Description

SABIC® SUPEER™ 8315 is an ethylene-octene copolymers produced via solution polymerization using metallocene catalyst. It performs well in a wide range of general purpose and high performance LLDPE cast film applications and has excellent impact strength and good transparency. SUPEER™ 8315 contains no slip and no antiblock additives.

This material data has been provided by Matmatch.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

0.92 g/cm³

Show Material materials with Density of 0.92 g/cm³

ASTM D1505

Thermal

PropertyValueComment

Melting point

113 °C

Show Material materials with Melting point of 113 °C

SABIC method

Optical

PropertyValueComment

Haze

1.5 %

Show Material materials with Haze of 1.5 %

ASTM D1003

Technological properties

Property
Application areas

Stretch film