SABIC® COHERE™ 8402

Want to keep this datasheet? Save it now in your required format

Description

SABIC® COHERE™ 8402 grade is an ethylene-octene copolymer produced via solution polymerization using metallocene catalyst. It performs well high performance LLDPE cast film and deliver outstanding toughness optics. SABIC® COHERE™ 8402 provides excellent performance as cling layer in stretch wrap film.

This material data has been provided by Matmatch.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyValueComment

Density

0.902 g/cm³

Show Material materials with Density of 0.902 g/cm³

ASTM D1505

Mechanical

PropertyValueComment

Elongation

850.0 %

Show Material materials with Elongation of 850.0 %

ASTM D638

Flexural modulus

0.0744799999999999 GPa

Show Material materials with Flexural modulus of 0.0744799999999999 GPa

ASTM D790

Tensile strength

19.6 MPa

Show Material materials with Tensile strength of 19.6 MPa

ASTM D638

Thermal

PropertyValueComment

Glass transition temperature

-32.0 °C

Show Material materials with Glass transition temperature of -32.0 °C

SABIC method

Melting point

100.0 °C

Show Material materials with Melting point of 100.0 °C

SABIC method

Optical

PropertyValueComment

Haze

0.5 %

Show Material materials with Haze of 0.5 %

ASTM D1003

Rheological Properties

PropertyValueComment

Mooney viscosity

10.0 MU

Show Material materials with Mooney viscosity of 10.0 MU

ASTM D1646 | ML 1+4, 121 °C

Technological properties

Property
Application areas

Stretch film,General purpose film,Lamination film