SABIC® LLDPE 118LJ

Want to keep this datasheet? Save it now in your required format

Description

118LJ is a butene Linear Low Density Polyethylene TNPP free grade suitable for general‐purpose blown films medium gauge. Films produced from these resins are tough with excellent puncture resistance, high tensile strength and good hot tack properties.

This material data has been provided by Matmatch.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

0.92 g/cm³

Show Material materials with Density of 0.92 g/cm³

ASTM D1505

Thermal

PropertyValueComment

Vicat softening temperature

100 °C

Show Material materials with Vicat softening temperature of 100 °C

ASTM D1525

Optical

PropertyValueComment

Haze

10 %

Show Material materials with Haze of 10 %

ASTM D1003

Technological properties

Property
Application areas

Stretch film,Shrink film,Blown film,General purpose film,Lamination film