SABIC® LLDPE 118NJ

Want to keep this datasheet? Save it now in your required format

Description

SABIC® LLDPE 118NJ is a butene linear low density polyethyleneresin typically used for general purpose applications. Films produced from this resin are tough with good puncture resistance, high tensile strength and good hot tack properties. 118NJ is TNPP free and it does not contain slip and antiblock additive.

This material data has been provided by Matmatch.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValueComment

Density

23.0 °C

0.92 g/cm³

Show Material materials with Density of 0.92 g/cm³

ASTM D1505

Mechanical

PropertyTemperatureValueComment

Tear strength

23.0 °C

40 kN/m

Show Material materials with Tear strength of 40 kN/m

ISO 6383-2

Tear strength, transverse

23.0 °C

120 kN/m

Show Material materials with Tear strength, transverse of 120 kN/m

ISO 6383-2

Optical

PropertyValueComment

Haze

13 %

Show Material materials with Haze of 13 %

ASTM D1003