SABIC® LLDPE 118WE

Want to keep this datasheet? Save it now in your required format

Description

SABIC® LLDPE 118WE is a butene-linear low density polyethylene resin for general purpose applications. Films produced from this resin are tough with excellent puncture resistance, high tensile strength, good hottack properties and low gel levels. The resin contains anti block and slip agent. Application Typical applications for SABIC® LLDPE 118WE are shipping sacks, ice bags, frozen food bags, liners, carrier bags, garbage bags, agriculture films, lamination and coextruded films, shrink film (for blending with LDPE), industrial consumer packaging and high clarity film if blended with (10-20%) LDPE. Film properties Film of 50 μm and BUR=2 has been produced on Kiefel IBC with 140 kg/h. Die size 200 mm, die gap 2,7 mm. The product mentioned

This material data has been provided by Matmatch.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValueComment

Coefficient of friction

0.1 [-]

Show Material materials with Coefficient of friction of 0.1 [-]

ASTM D1894

Density

23.0 °C

0.92 g/cm³

Show Material materials with Density of 0.92 g/cm³

ASTM D1505

Mechanical

PropertyTemperatureValueComment

Tear strength

23.0 °C

40 kN/m

Show Material materials with Tear strength of 40 kN/m

ISO 6383-2

Tear strength, transverse

23.0 °C

120 kN/m

Show Material materials with Tear strength, transverse of 120 kN/m

ISO 6383-2

Optical

PropertyValueComment

Haze

20 %

Show Material materials with Haze of 20 %

ASTM D1003

Technological properties

Property
Application areas

Shipping sacks, ice bags, frozen food bags, liners, carrier bags, garbage bags, agriculture films, lamination and coextruded films, shrink film (for blending with LDPE), industrial consumer packaging and high clarity film if blended with (10-20%) LDPE.