SABIC® LLDPE 118WJ

Want to keep this datasheet? Save it now in your required format

Description

SABIC® LLDPE 118WJ is a butene linear low density polyethylene resin typically used for general purpose applications. Films produced from this resin are tough with good puncture resistance, high tensile strength and good hottack properties. The resin contains slip and antiblock additive. SABIC® LLDPE 118WJ is TNPP free. This product is not intended for and must not be used in any pharmaceutical/medical applications.

This material data has been provided by Matmatch.

All metrics apply to room temperature unless otherwise stated. SI units used unless otherwise stated.
Equivalent standards are similar to one or more standards provided by the supplier. Some equivalent standards may be stricter whereas others may be outside the bounds of the original standard.

Ashby charts

Properties

General

PropertyTemperatureValueComment

Coefficient of friction

0.1 [-]

Show Material materials with Coefficient of friction of 0.1 [-]

ASTM D1894

Density

23.0 °C

0.92 g/cm³

Show Material materials with Density of 0.92 g/cm³

ASTM D1505

Mechanical

PropertyTemperatureValueComment

Tear strength

23.0 °C

40 kN/m

Show Material materials with Tear strength of 40 kN/m

ISO 6383-2

Tear strength, transverse

23.0 °C

120 kN/m

Show Material materials with Tear strength, transverse of 120 kN/m

ISO 6383-2

Optical

PropertyValueComment

Haze

20 %

Show Material materials with Haze of 20 %

ASTM D1003